| 硼在钢中的分布 |
| 贺信莱;褚幼义;张秀林;余宗森;李秋萍;尹熙光 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院;北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
| THE DISTRIBUTION OF BORON IN STEEL |
| Ho Hsin-lai;Chu Yu-yi;Chang Hsiu-lin;Yu Tsung-sen;Li Chiu-ping (student);Yin Hsi-kuang (student) Peking Institute of Iron and Steel Technology |
引用本文:
贺信莱;褚幼义;张秀林;余宗森;李秋萍;尹熙光. 硼在钢中的分布[J]. 金属学报, 1977, 13(4): 235-356.
,
,
,
,
,
.
THE DISTRIBUTION OF BORON IN STEEL[J]. Acta Metall Sin, 1977, 13(4): 235-356.
[1] Armijo, J. S. and Rosenbaum, H. S., J. Appl. Phys., 38 (1967) , 2064. [2] Williams, T. M. et. al., Metal Sci. J., 10 (1976) , 14. [3] Adair, A. M. et al., Trans. AIME, 203 (1955) , 353. [4] Aust, K. T. et al., Acta Met., 16 (1968) , 291. [5] Jandeska, W. F. Jr. and Morral, J. E., Met. Trans., 3 (1972) , 2933. [6] #12. [7] #12. |
|