| 定量测定晶粒取向及织构的蚀坑法 |
| 罗阳 |
|
| QUANTITATIVE DETERMINAMON OF GRAIN ORIENTATION AND TEXTURE BY ETCH-FIGURE METHOD |
| Luo Yang |
引用本文:
罗阳. 定量测定晶粒取向及织构的蚀坑法[J]. 金属学报, 1977, 13(z1): 93-108.
.
QUANTITATIVE DETERMINAMON OF GRAIN ORIENTATION AND TEXTURE BY ETCH-FIGURE METHOD[J]. Acta Metall Sin, 1977, 13(z1): 93-108.
[1] Mueller, M. H. et al., Rev. Sci. Instrum., ?as (1954) , 1115. [2] Illgeh, L. et al., Prakt. Metall?gr., 6 (1969) , 363. [3] Tassy-Betz, E. et al, Metallography, 7 (1974) , 1. |
|