Please wait a minute...
金属学报  1978, Vol. 14 Issue (1): 17-26    
  论文 本期目录 | 过刊浏览 |
混合甲苯胂酸浮选锡石的研究
No Author
长沙矿冶研究所浮锡组
AN INVESTIGATION OF CASSITERITE FLOTATION USING MIXED TOLYL ARSONIC ACID
Res. Gp. of Cassiterite Flotation; Changsha Institute of Mining and Metallurgy Research
引用本文:

No Author. 混合甲苯胂酸浮选锡石的研究[J]. 金属学报, 1978, 14(1): 17-26.
. AN INVESTIGATION OF CASSITERITE FLOTATION USING MIXED TOLYL ARSONIC ACID[J]. Acta Metall Sin, 1978, 14(1): 17-26.

全文: PDF(673 KB)  
摘要: 本文介绍了用混合甲苯胂酸浮选锡石的研究工作,试验表明混合甲苯胂酸对锡石的捕收能力优于对位和邻位甲苯胂酸。当混合比为45:55时,锡石产率出现“峰值”,可得到较高的浮选指标。为降低药剂成本,利用化工厂废弃的冷母液制造混合甲苯胂酸,在工业生产中证明是十分成功的。
Abstract:The capacity of tolyl arsonic acids for collecting cassiterite has been investigated. It is shown that mixed tolyl arsonic acid was much superior to either para- or ortho-isomer alone for cassiterite flotation. Mixing ratios between paraand ortho-tolyl arsonic acids ranging from 50:50 to 30:70 were effective with a peak value at 45:55 in which a maximum collecting capacity was obtained. The preparation of mixed tolyl arsonic acid was more convenient than that of paraisomer, a conventional collecting agent for cassiterite flotation. In the plantscale flotation of cassiterite slimes assaying from 0.6 to 0.7 percent Sn, tin concentrates with the grade of about 25.65% were obtained, the total recovery being about 58.64%. Cassiterite flotation using mixed tolyl arsonic acid as collectors and sodium carbonyl methyl cellulose as despressing agents for calcite have already been put into industrial practice.
收稿日期: 1978-01-18     
[1] Topfer, E., Freiber. Forschungsh., [Reihe] A163 (1960) , 63.