| 一种35Ni-15Cr型铁基高温合金的氧化、腐蚀与防护 |
| 郭建亭 |
| 中国科学院金属研究所 |
|
| AN INVESTIGATION OF THE OXIDATION AND HOT CORROSION OF A 3SNi-15Cr TYPE IRON-BASE ALLOY |
| Guo Jianting Institute of Metal Research; Academia Sinica |
引用本文:
郭建亭. 一种35Ni-15Cr型铁基高温合金的氧化、腐蚀与防护[J]. 金属学报, 1979, 15(2): 203-305.
.
AN INVESTIGATION OF THE OXIDATION AND HOT CORROSION OF A 3SNi-15Cr TYPE IRON-BASE ALLOY[J]. Acta Metall Sin, 1979, 15(2): 203-305.
[1] Kubaschewski, O. and Hopkins, B. E., Oxidation of Metals and Alloys, 2nd ed., Butterworths, London, 1962, p. 49. [2] 铁基高温合金研究组,金属学报,14(1978) ,227. [3] 铁基高温合金研究组,金属学报,14(1978) ,348. [4] Hagel, W. C. and Seybolt, A. U., J. Electrochem. Soc., 108 (1961) , 1146. [5] Himmel, L., Mehl, R. F. and Birchenall, C. E., J. Metals, 5 (1953) , 827. [6] 郭建亭,朱耀宵,师昌绪,金属学报,10 (1974) , 74. [7] Wlodek, S. T., Trans. AIME, 230 (1964) , 177. [8] ibid, 230 (1964) , 1078. [9] Rhee, S. K. and Spencer, A. R., Met Trans., 1 (1970) , 2021. [10] Stringer, J., Annual Review of Materials Science, Vol. 7, Palo Alto, California, 1977, p. 477. [11] Bergman, P. A., Corrosion, 23 (1967) , № 3, 72. [12] 姚鸿年,金相研究法,中国工业出版社, 1963, p. 374. [13] Paladino, A. E. and Kingery, W. D., J. Chem. Phys., 37 (1962) , 957. [14] Nicholls, B. J., Corros. Technol., 9 (1962) , № 9, 238. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|