| 稀土元素对Fe-Cr-Al合金高温氧化层残余应力的影响 |
| 张立新;李黎光;银耀德;赵齐;张丙申 |
|
| AN INVESTIGATION OF RESIDUAL STRESS OF OXIDE SCALE AFFECTED BY THE ADDITION OF RARE EARTH ELEMENTS IN Fe-Cr-Al ALLOY AT 1200 AND 1350℃ |
| Zhang Lixin;Li Liguang;Yin Yaode;Zhao Qi;Zhang Bingshen |
引用本文:
张立新;李黎光;银耀德;赵齐;张丙申. 稀土元素对Fe-Cr-Al合金高温氧化层残余应力的影响[J]. 金属学报, 1980, 16(4): 411-419.
,
,
,
,
.
AN INVESTIGATION OF RESIDUAL STRESS OF OXIDE SCALE AFFECTED BY THE ADDITION OF RARE EARTH ELEMENTS IN Fe-Cr-Al ALLOY AT 1200 AND 1350℃[J]. Acta Metall Sin, 1980, 16(4): 411-419.
[1] Wukusick, C. S., and Collins, J. F., Mater. Res. Stand. 4 (1964) , 637. [2] Stringer, J., Met. Rev., 11 (1966) , 113. [3] Tien, J. K. and Pettit, F. S., Met. Trans. 3 (1972) , 1578. [4] Pfeiffer, V. H., Werkst. Korros., 8 (1957) , 574. [5] Frances, J. M. and Jutson, J. A., Corros. Sci., 8 (1968) , 445. [6] Golightly, F. A., Stott, F. H. and Wood, G. C., Oxid. Metals, 10 (1976) , 163. [7] Douglass, P. L., Oxidation of Metals and Alloys, Paper presented at a seminar of the ASM. l970, Oct., Metals Park, Ohio, 1971, p. 137. [8] 骆继勋,银耀德,林生昆,赵齐,王俭,金属学报,13(1977) ,263. [9] Klug, H. P. and Alexander, L. E., X-Ray Diffraction Procedures for Polycrystalline and Amorphous Materials, 2nd ed., Wiley, New York, 1974, p. 761. [10] Ibid., p. 302. [11] Mar, H. Y. B. and Scott, W. D., J. Amer. Cer. Soc. 53 (1970) , 555. [12] 待发表工作. [13] 章复中,孙传岳,金属学报,16(1980) .394. [14] 李碚,骆继群,于洪香,金属学报,16(1980) .401 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|