| 立方晶体中<100>,<110>,<111>方向椭圆柱形夹杂物弹性能数值解 |
| 颜本达;吴建生;林栋梁;周以苍 |
| 上海交通大学;上海交通大学;上海交通大学;美国里海大学冶金及材料工程系;上海交通大学兼任教授 |
|
| NUMERICAL SOLUTION OF ELASTIC ENERGY OF ELLIPTIC INCLUSIONS ORIENTED IN <100>,<110>AND <111> DIRECTIONS IN CUBIC CRYSTALS |
| by Yah Benda; Wu Jiansheng and Lin Dongliang (T. L. Lin) (Shanghai Jiaotong University) and Y. T. Chou (Department of Metallurgy and Materials Science; Leihigh University; U. S. A.; Adjunct Professor in Shanghai Jiaotong University; China) |
引用本文:
颜本达;吴建生;林栋梁;周以苍. 立方晶体中<100>,<110>,<111>方向椭圆柱形夹杂物弹性能数值解[J]. 金属学报, 1981, 17(5): 489-505.
,
,
,
.
NUMERICAL SOLUTION OF ELASTIC ENERGY OF ELLIPTIC INCLUSIONS ORIENTED IN <100>,<110>AND <111> DIRECTIONS IN CUBIC CRYSTALS[J]. Acta Metall Sin, 1981, 17(5): 489-505.
[1] Eshelby, J. D., Progress in Solid Mechanics, Ed. by I. N. Snedden and R. Hill, North Holland, Vol. 2, 1961, p. 89. [2] Eshelby, J. D., Proc. R. Soc. London, Ser. A, 241 (1957) , 376. [3] Eshelby, J. D., Proc. R. Soc. London, Ser. A, 252 (1959) , 561. [4] Jaswon, M. A. and Bhargava, R, D., Proe. Cambridge Philos. Soc. 57 (1961) , 669. [5] Willis, J. R., Q. J. Mech. Appl. Math., 17 (1964) , 157. [6] Bhargava, R. D. and Rodhakrishna, H. C., J. Phys. Soc. Jpn., 19 (1964) , 396. [7] Chen, W. T., Q. J. Mech. Appl. Math., 20 (1967) , 307. [8] Walpole, L. J., Proc. R. Soc. London, Ser. A, 300 (1967) , 270. [9] Yang, H. C. and Chou, Y. T., Trans. ASME, Ser. E: J. Appl. Mech., 43 (1976) , 424. [10] Eshelby, J. D., Read, W. T. and Shockley, W., Acta Metall., 1 (1953) , 251. [11] Stroh, A. N., Philos. Mag., 3 (1958) , 625. [12] Yang, H, C. and Chou, Y. T., Mater. Sci. Eng., 17 (1975) , 57. [13] Head, A. K., Humble, P., Clarebrough, L. M., Morton, A. J. and Porwood, C. T., Computed Electron Micrographs and Defect Identification, 1973, p. 126. [14] Bacon, D. J., Barnett, D. M. and Scattergood, R. O., Prog. Mater. Sci., 23 (1978) , 162. [15] 冯端,金属物理(下册),科学出版社,1975,p.527. [16] Shibata, M. and Ono, K., Acta Metall, 23 (1975) , 587. [17] Mura, T. and Lin, S. C., Trans. ASME, Set E: J. Appl. Mech., 41 (1974) , 209. [18] Chou, Y. T., Lin, T. L. and Wu, J. S., to be published, 1981 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|