| 关于氧化物固溶体相变消除问题 |
| 郁国城 |
| 冶金工业部洛阳耐火材料研究所 |
|
| ON THE ELIMINATION OF POLYMORPHISM OF OXIDE SOLID SOLUTIONS |
| by Yu Guocheng (Luoyang Institute of Refractory Research) |
引用本文:
郁国城. 关于氧化物固溶体相变消除问题[J]. 金属学报, 1981, 17(5): 578-582.
.
ON THE ELIMINATION OF POLYMORPHISM OF OXIDE SOLID SOLUTIONS[J]. Acta Metall Sin, 1981, 17(5): 578-582.
[1] Levin, J. and Otte, E., J. Am. Chem. Soc., 54 (1932) , 828. [2] Greig, J. W., ibid., 54 (1932) , 2846. [3] 陈显求,金属学报,2(1957) ,99. [4] Klasik, J. A., Science, 189 (1975) , 631. [5] Moetel, H. and Paetsch, D., Ber. Dtsch. Keram. Ges., 52 (1975) 8. [6] Ruff, O. and Ebert, F., Z. Anorg. Allgem. Chem., 180 (1929) , 19. [7] Clark, G. L. and Reynolds, D. H., Ind. Eng. Chem., 29 (1937) 711. [8] Cypres, R., Wollast, R. und Raucq, J., Ber. Dtsch. Keram. Ges., 40 (1963) , 527, [9] Clearfield, A., Inorg, Chem., 3 (1964) , 146. [10] Garvie, R. C., J. Phys. Chem., 69 (1965) , 1238. [11] Garvie, R. C., Hannink, R. H. and Pascoe, R. T., Nature, 258 (1975) , 703, [12] Whitney, E. D., Trans. Faraday Soc., 61 (1965) , 1991. [13] Mitsuhashi, T., Ichihara, M. and Tatsuke, U., J. Am. Ceram. Soc., 57 (1974) , 97. [14] 姜铃章,陈士萍,陈显求,包单吾,黄渊莉,戴玉龙,涂淑进,未发表资料,1978. [15] Hauth, W. E., Jr., Am. Ceram. Soc. Bull., 30 (1951) , 165. [16] Koehler, E. K., and Glushkova, V. B., Science Ceramic, Vol. 4, Ed. by G. H. Stewart, Brit, Ceram. Soc., 1968, P. 233. [17] Spitzbergen, U. and Houpt, P. M., ibid., P. 247. [18] Duwez, P. and Odell, F., J. Am. Ceram. Soc., 33 (1950) , 274. [19]#12m |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|