| Zr对Fe-Ni-Co-Cu系合金晶粒长大及性能的影响 |
| 马莒生 |
| 清华大学 |
|
| THE EFFECT OF Zr ON THE GRAIN GROWTH BEHAVIOUR AND PROPERTIES OF Fe-Ni-Co-Cu TYPE ALLOYS |
| Ma Jusheng (Tsinghua University; Beijing) |
引用本文:
马莒生. Zr对Fe-Ni-Co-Cu系合金晶粒长大及性能的影响[J]. 金属学报, 1982, 18(1): 64-131.
.
THE EFFECT OF Zr ON THE GRAIN GROWTH BEHAVIOUR AND PROPERTIES OF Fe-Ni-Co-Cu TYPE ALLOYS[J]. Acta Metall Sin, 1982, 18(1): 64-131.
1 Ciriack, G., Metall., 24 (1970) , 472. 2 Elliott, R. P., Constitution of Binary Alloys, First Suppl, McGraw-Hill, 1965, p. 679. 3 #12 4 潘金生,未发表资料,1980. 5 久保寺治朗;中岡一郎;须田豊治,日本金属学会誌,31(1967) ,527. 6 足立彰;水川消;大本裕万;平岡异,铁钢,44(1958) ,1192. 7 足立彰;水川清;铁纲,48(1962) ,683. 8 藤田清比古,盛利贞;津岛健冶;平沢良和;福井敞,铁纲,59(1973) ,929. 9 Gladman, T.; Dulieu, D., Met. Sci., 8 (1974) , 167. 10 颜呜皋,周邦新,物理学报,2(1958) ,121. |
|