| 沉淀强化镍基高温合金中γ′相数量的计算表达式 |
| 杨洪才 |
| 东北工学院 |
|
| A FORMULA FOR γ′-PHASE AMOUNTING IN PRECIPITATION HARDENING NICKEL-BASE SUPERALLOYS |
| Yang Hongcai (Northeast Institute of Technology; Shenyang) (Manuscript received 13 April; 1981) |
引用本文:
杨洪才. 沉淀强化镍基高温合金中γ′相数量的计算表达式[J]. 金属学报, 1982, 18(4): 510-514.
.
A FORMULA FOR γ′-PHASE AMOUNTING IN PRECIPITATION HARDENING NICKEL-BASE SUPERALLOYS[J]. Acta Metall Sin, 1982, 18(4): 510-514.
1 Woodyatt, L.R.; Sims, C.T.; Beattie, H.J., Trans. Metall. Soc. AIME, 236(1966) , 519. 2 Dreshfieid, R.L.; Wallace, J.F., NASA-CR-120 940,(1972) ,P.134. 3 Krige, O.H., ASM Trans. Q., 62(1969) , 195. 4 渡辺力藏,九重常男,铁鋼,61(1975) ,2277. 5 Watanabe, R.; Kuno, T., Trans. Iron Steel Inst. Jpn., 16(1976) , 439. 6 Decker, R.F.; Sims, C.T., The Superalloys, Eds. Sims, C.T.; Hagel, W.C., Wiley New York, 1972, p.33. 7 #12 8 #12 |
|