| 等温处理过程中BN的析出行为 |
| 尹士科;小松肇;谷野满 |
| 冶金工业部钢铁研究总院;日本新日本制铁(株)基础研究所;日本新日本制铁(株)基础研究所 |
|
| THE PRECIPITATION OF BN IN ISOTHERMAL TREATMENT PROCESS |
| Yin Shike (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Belling); Hajime Komatsu; Mitsuru Tanino (Fundamental Research Laboratories; Nippon Steel Corporation; Japan) |
引用本文:
尹士科;小松肇;谷野满. 等温处理过程中BN的析出行为[J]. 金属学报, 1982, 18(5): 565-646.
,
,
.
THE PRECIPITATION OF BN IN ISOTHERMAL TREATMENT PROCESS[J]. Acta Metall Sin, 1982, 18(5): 565-646.
1 尹士科;小松肇;谷野满,金属学报,18(1982) ,565. 2 渡迈征一;大谷泰夫,铁钢,62(1976) ,1851 |
|