| Gd-Co-Ni三元系相图 |
| 郑建宣;徐国雄 |
| 广西大学;广西大学 |
|
| A PART OF PHASE DIAGRAM OF Gd-Co-Ni SYSTEM |
| ZHENG Jianxuan; XU Guoxiong (Guangxi University; Nanning) |
引用本文:
郑建宣;徐国雄. Gd-Co-Ni三元系相图[J]. 金属学报, 1983, 19(1): 9-11.
,
.
A PART OF PHASE DIAGRAM OF Gd-Co-Ni SYSTEM[J]. Acta Metall Sin, 1983, 19(1): 9-11.