陈肇友. 从相图剖析炉渣对MgO-CaO材料的侵蚀[J]. 金属学报, 1983, 19(2): 106-113.
.
APPLICATION OF PHASE DIAGRAMS TO SLAG ATTACK ON MgO-CaO REFRACTORIES[J]. Acta Metall Sin, 1983, 19(2): 106-113.
1 Troemel, G.; Obst, K.-H; Goerl, E,; Stradtmann, J., Tonind.-Ztg., 90 (1966) , 193. 2 #12 3 Nafziger, R. H., High Temp. Sci., 7 (1975) , 179. 4 Levin, E. M.; Robbins, C. R.; McMurdie, H. F., Phase Diagrams for Ceramists, Second Edition, 1969, p. 209, 210, 113; Phase Diagrams for Ceramists, 1969 Supplement, p. 36, 85. 5 Johnson, R. E.; Muan, A.; J. Am. Ceram. Soc., 48 (1965) , 359. 6 Stephenson, I. M.; White, J., Trans. Br. Ceram. Soc., 66 (1967) , 443. 7 Troemel, G.; Fix, W.; Kaup. R., Arch. Eisenhuettenwes., 38 (1967) , 595. 8 Drewes, E. J.; Olette, M., ibid. 38 (1967) , 163. 9 Troemel, G.; Fix, W.; Koch, K., ibid., 38 (1967) , 177. 10 Knueppel, H.; Oeters, F., Stahl Eisen, 81 (1961) , 1437. 11 郁国城,金属学报,14(1978) ,272. 12 Troemel, G.; Koch, K., Arch. Eisenhuettenwes., 45 (1974) , 671. 13 Euler, R., Ber. Dtsch. Keram. Ges., 44 (1967) , 345.9 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|