金属学报  1983, Vol. 19 Issue (3): 16-22    
  论文 本期目录 | 过刊浏览 |
近零磁伸非晶环样磁滞回线的偏移和消除方法
陈笃行;潘孝硕
中国科学院物理研究所;冶金工业部钢铁研究总院;中国科学院物理研究所
SHIFT OF HYSTERESIS LOOPS FOR NEARLY ZERO- MAGNETOSTRICTIVE NON-CRYSTALLINE TOROIDAL SAMPLES AND ITS ELIMINATING METHODS
by CHEN Duxing; PAN Xiaoshuo (Institute of Physics; Academia Sinica; Beijing)
引用本文:

陈笃行;潘孝硕. 近零磁伸非晶环样磁滞回线的偏移和消除方法[J]. 金属学报, 1983, 19(3): 16-22.
, . SHIFT OF HYSTERESIS LOOPS FOR NEARLY ZERO- MAGNETOSTRICTIVE NON-CRYSTALLINE TOROIDAL SAMPLES AND ITS ELIMINATING METHODS[J]. Acta Metall Sin, 1983, 19(3): 16-22.

全文: PDF(557 KB)  
摘要: 通过几个近零磁伸非晶环样磁滞回线的偏移随测前磁操作变化的实验研究,指出经过420℃以上退火的样品,磁滞回线的偏移与非晶母体内析出高H_c微晶有关,而通过适当的退磁和冲击磁化的操作,可以不同程度地消除偏移,消偏磁滞回线的H_c随所用磁操作而变。
Abstract:Several nearly zero-magnetostrictive non-crystalline toroidal samples have been examined for the shift of hysteresis loops changed by the magnetic operations prior to their measurements. It is shown that the loop shift of the samples annealed over 420℃ is related to the precipitation of crystallites with high H_c from the non-crystalline matrix. It can be eliminated to a certain extent by means of some suitable demagnetizing or shock-magnetizing, and the H_c of the shift-eliminated loops varies with the operations preformed.
收稿日期: 1983-03-18     
1 Kohmoto, O., Yamaguchi, N.;Ohya,K; Fujishima, H., Jpn. J. Appl. Phys., 17 (1978) , 257.
2 高桥実;宫崎照宣;渡部明夫,日本金属学会讲誌,43(1979) ,339.
3 Ohta, K.; Matsuyama, T., Kajiura,M.; Teranishi, T., J. Magn. Magn. Mater., 19 (1980) , 165.