| 晶格稳定参数的确定和应用 |
| 王明贤 |
| 中国科学院金属研究所 |
|
| DETERMINATION OF LATTICE STABILITY PARAMETERS AND THEIR APPLICATION |
| by WANG Mingxian (Institute of Metal Research; Academia Sinica; Shenyang) |
引用本文:
王明贤. 晶格稳定参数的确定和应用[J]. 金属学报, 1983, 19(3): 106-111.
.
DETERMINATION OF LATTICE STABILITY PARAMETERS AND THEIR APPLICATION[J]. Acta Metall Sin, 1983, 19(3): 106-111.
1 Kaufman, L., Metallurgical Chemistry, NPL, England, 1972, p. 375. 2 Ansara, I., Int. Met. Rev., 1 (1979) , 25. 3 Hillert, M., Calculation of Phase Diagrams and Thermochemistry of Alloy Phases, The Metall. Soc. of AIME, 1979, p. 3. 4 Hultgren, R., Selected Values of the Thermodynamic Propertes of Binary Alloys, ASM, 1973, p. 1277. 5 Hultgren, R. ibid., p. 1280. 6 Hultgren, R., Selected Values of Thermodynamic Properties of the Elements, ASM, 1973, p. 526. 7 Hultgren, R., ibid., p. 382. 8 王明贤,雷琼芝,金属学报,18(1982) ,627. 9 Hultgren, R., Selected Values of the Thermodynamic Properties of Binary Alloys, ASM,1973, p. 45. 10 Hultgren, R., ibid., p.47. 11 Michaels, K. F.; Lange, W. F.; Bradley, J. R.; Aaronson, H. I., Metall. Trans., 6A (1975) , 1843. 12 徐祖耀,金属学原理,上海科学技术出版社,1963. p.217. 13 徐祖耀,金属材料热力学,科学出版社 1981. p.210,276. 14 Jantzen, C. M. F.; Herman, H., Phase Diagrams, Materials Science and Technology, Ed. Alper, A, M., Vol. 5, 1978, p. 155. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|