| VIA族元素在Ti中的最大固溶度变化规律及Po的有效电荷计算 |
| 王孔探 |
| 洛阳船舶材料研究所 |
|
| MAXIMUM SOLUBILITY VARIATION OF ELEMENTS OF GROUP VIA IN Ti AND CALCULATION OF EFFECTIVE ELECTRIC CHARGE OF Po |
| by WANG Kongtan (Luoyang Ship Material Research Institute) |
引用本文:
王孔探. VIA族元素在Ti中的最大固溶度变化规律及Po的有效电荷计算[J]. 金属学报, 1983, 19(3): 118-122.
.
MAXIMUM SOLUBILITY VARIATION OF ELEMENTS OF GROUP VIA IN Ti AND CALCULATION OF EFFECTIVE ELECTRIC CHARGE OF Po[J]. Acta Metall Sin, 1983, 19(3): 118-122.