| 09MnNb钢低温下的冲击断裂行为 |
| 蔡体刚;李培良;蒋景凯 |
| 包头冶金研究所;包头冶金研究所;包头冶金研究所 |
|
| IMPACT FRACTURE BEHAVIOUR OF 09MnNb STEEL AT LOW TEMPERATURES |
| by CAI Tikang; LI Peiliang; JIANG Jingkai (Baotou Institute of Metallurgy) (Manuscript received 10 January; 1981; revised manuscript 4 December; 1982) |
引用本文:
蔡体刚;李培良;蒋景凯. 09MnNb钢低温下的冲击断裂行为[J]. 金属学报, 1983, 19(4): 88-152.
,
,
.
IMPACT FRACTURE BEHAVIOUR OF 09MnNb STEEL AT LOW TEMPERATURES[J]. Acta Metall Sin, 1983, 19(4): 88-152.