弱磁材料测量中由退磁场引起的误差
陈笃行;李伯臧
北京冶金研究所;北京冶金研究所
ON THE ERROR OF MEASUREMENT OF FEEBLY MAGNETIC MATERIAL IN REGARD TO DEMAGNETIZING FIELD
CHEN Duxing; LI Bozang (Beijing Research Institute of Metallurgy)
引用本文:

陈笃行;李伯臧. 弱磁材料测量中由退磁场引起的误差[J]. 金属学报, 1983, 19(5): 141-148.
, . ON THE ERROR OF MEASUREMENT OF FEEBLY MAGNETIC MATERIAL IN REGARD TO DEMAGNETIZING FIELD[J]. Acta Metall Sin, 1983, 19(5): 141-148.

全文: PDF(597 KB)  
摘要: 现有的一些弱磁材料标准测磁方法,忽视了退磁场对冲击法磁化强度测量的重要影响,因而给出了过于乐观的精度估计。本文分析了退磁场对弱磁测量的影响,计算了无磁圆柱样品关于样品和线圈的冲击退磁因子,给出了退磁场引起的磁场、磁化强度测量误差及其修正办法,对弱磁测置的标准尺寸提出了建议。
Abstract:An over-optimistic assessment in accuracy is often resulted from the magnetization measurement by the current standard methods for the feebly magnetic materials due to ignoring the significant influence of demagnetizing field on the ballistic method. Analysis is reported on the effect of demagnetizing field upon the feebly magnetic measurement, and calculation is presented to two kinds of ballistic demagnetizing factors which are about non-magnetic cylindrical specimen itself and about its measuring coil. Thus, the errors of H and M measurements in regard tO the demagnetizing field and their correct method as well are given. It may be suggested that a set of standard dimensions for the feebly magnetic measurement is available.
收稿日期: 1983-05-18     
1 ASTM A342-64 (1970) , 1971 Annual Book of ASTM Standards, Part 8, ASTM, 1971, p. 38.
2 直流与交流磁测量,刘湘元等译,上海科学技术出版社,1964,p.100.
3 Bozorth, R. M., Ferromagnetism, D. Van Nostrand Co., 1956, p. 846.
No related articles found!