| 电渣重熔对一种Co基高温合金晶界化学成分的影响 |
| 戴彤孚;王淑荷;师昌绪 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| EFFECT OF ESR ON CONSTITUTION NEARBY GRAIN BOUNDARY IN A Co-BASE SUPERALLOY |
| DAI Tongfu; WANG Shuhe; SHI Changxu (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 2 August; 1982; revised manuscript 25 January;1983) |
引用本文:
戴彤孚;王淑荷;师昌绪. 电渣重熔对一种Co基高温合金晶界化学成分的影响[J]. 金属学报, 1984, 20(1): 47-148.
,
,
.
EFFECT OF ESR ON CONSTITUTION NEARBY GRAIN BOUNDARY IN A Co-BASE SUPERALLOY[J]. Acta Metall Sin, 1984, 20(1): 47-148.
1 Bhat, G, K.; Tobias, J.B.; Kennard, R.L., Second International Symposium on Electroslag Remelting Technology, Symp. Proc. Part one, Ed. Bhat, G.K., Pennsylvania, 1969. 2 #12 3 Heslop, J.; Knott, A.R., Met. Mater., 5 (1971) , No. 2, 59. 4 #12 5 Mclean, D., Grain Boundaries in Metals, Oxford, 1957, pp. 116--149. 6 Handbook of Auger Electron Spectroscopy, 2nd, Ed. Palmberg, P.W., Phys. Electr. Ind. Inc., Minnesota, 1976, pp. 5-10. 7 Aerospace Structural Metals Handbook, Eds. Wolf. J.; Brown, Jr., W.F., Belfour Stulen Inc., Watertown, Mass., 1975, Code 4310. 8 #12 9 Walsh, J. M; Anderson, N.P., Superalloys-Metallurgy and Manufacture, Proc. of the Ⅲ Int. Symp., Eds. Kear, B.H.; Muzyka, D.R., et al., Baton Rouge Clator's Publ., 1976, pp. 127-136 10 Yamagnchi, S., Met. Technol, 6 (1979) , 170. 11 曲哲,郭可信,金图学报,16(1980) ,371./ |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|