| 交流电渣重熔过程中的成分变化——Ⅰ.理论传质模型 |
| 魏季和;A.Mitchell |
| 西安冶金建筑学院;加拿大不列颠哥伦比亚大学 |
|
| CHANGES IN COMPOSITION DURING A. C. ESR——Ⅰ. Theoretical Development |
| WEI Jiho (Wei Chi-ho)(Xi'an Institute of Metallurgy and Construction Engineering); MITCHELL A. (University of British Columbia; Vancouver; B. C. ; Canada) (Manuscript received 27 May; 1983) |
引用本文:
魏季和;A.Mitchell. 交流电渣重熔过程中的成分变化——Ⅰ.理论传质模型[J]. 金属学报, 1984, 20(5): 387-405.
,
.
CHANGES IN COMPOSITION DURING A. C. ESR——Ⅰ. Theoretical Development[J]. Acta Metall Sin, 1984, 20(5): 387-405.
1 Hawkins, R. J. ; Meherali, S. G. ; Davies, M. W. , J. Iron Steel Inst. , 209 (1971) , 646. 2 Hawkins, R. J. ; Swinden, D. J. ; Pocklington, D. N. , Electroslag Relining, The Iron & Steel Inst. , London, 1973, p. 21. 3 Knights, C. F. , Perkins, R. , ibid. , p. 35. 4 Hoyle, G. ; Dewsnap, P. ; Salt, D. J. ; Barrs, E. M. , Electro-Slag Relining Technology, BISRA, Open Rep. No. MG/A/416/66/1966, London, Br. Iron & Steel Res. Association. 5 Davis, M. W. ; Hawkins, R. J. ; Smith, P. N. , Steel Times, 197 (1969) , 237; 353. 6 Pateisky, G. ; Biele, H. ; Fleisher, H. J. , J. Vac. Sci. Technol. , 9 (1972) , 1318. 7 Schmidt, M. , Private communication. 8 Elienne, M. , Ph. D. Thesis, University of British Columbia, 1970. 9 Etienne, M. ; Mitchell, A. , Electr. Furnace Conf. Proc. , 28 (1970) , p. 28. 10 Fraser, M. E. , Ph. D. Thesis, University of British Columbia, 1974. 11 Fraser, M. E. ; Mitchell, A. , Ironmaking Steelmaking, 3 (1976) , №5, 279; 288. 12 Schwerdtfeger, K. ; Wepner, W. ; Pateisky, G. , ibid. , 5 (1978) , №3, 135. 13 Cooper, C. K. , Ghosh, D. : Kay, D. A. R. ; Pomfret, R. J. , Electr. Furnace Conf. Proc. , 28 (1970) , 8. 14 #12 15 Mitchell, A. ; Szekely, J. ; Elliott, J. F. , Electroslag Refining, The Iron Steel Inst. , 1973, London, p .3. 16 Mitchell, A. , Int. Symp. on Metallurgical Slags, C. I. M. M. , Halifax N. S. , August, 1980, Section 7. 17 Mitchell, A. , ES & VA Remelting, to be published. 18 Allibert, M. ; Wadier, J. F. ; Mitchell, A. , Ironmaking Steelmaking, 5 (1978) , №5, 211. 19 Wei Chi-ho (魏季和); Mitchell, A. , Deoxidation in ESR, to be published. 20 Miska, H. , Dissertation, Technical University Ciausthal, 1971. 21 Mitchell, A. ; Jackson, R. O. ; Ballantyne, A. S. , Proc. 4th Int. Symp. on ESR Processes, ISIJ, Tokyo, 1973, p. 1. 22 Chipman, J. , Basic Open Hearth Steelmaking, Ed. Derge, G. , 3rd ed. , AIME, 1964, p. 531. 23 Elliott, J. F. ; Gleiser, M. ; Ramakrishna, V. , Thermochemistry for Steelmaking, Vol. Ⅱ, Addison-Wesley, USA, 1963, p. 621, 702. 24 Sigworth, G. K. ; Elliott, J. F. , Met. Sci. J. , 8 (1974) , 298. 25 Kusuhiro, M. ; Uchida, A. ; Tagami, T. ; Wasai, Y. , Proc. 3rd Int. Iron & Steel Congress, April, 1978, Chicago, Illinois, ASM and Iron & Steel Soc. of AIME, Ohio, 1979, p. 266. 26 Schenck, H. ; Steinmetz, E. , Wirkungsparmeter von Begleitelementen Flussiger Eisenlosungen und Gegenseitigen Beziehungen, 2. Aufl. Verlag Stahl und Eisen, Dusseldorf, 1968. 27 Korousic, B. , Berg-und Huttnmannische Monatshefte, 122 (1977) , №7, 287. 28 Kubaschewski, O. ; Alcock, C. B. , Metallurgical Thermochemistry, 5th ed. , Pergamon Press, 1979, p. 381. 29 Turkdogan, E. T. , Physical Chemistry of High Temperature Technology, Academic Press, 1980, p. 381. 30 Mclean, A. ; Ward, R. G. , J. Iron Steel Inst. , 204 (1966) , 8. 31#12 32 Jackson, R. O. , M. A. Sc. Thesis, University of British Columbia, 1971. 33 Mitchell, A. ; Joshi, S. , Metall. Trans. , 4 (1973) , 631. 34 Mellberg, P. O. , Proc. 4th Int. Symp. on ESR Processes, ISIJ, Tokyo, 1973, p. 13. 35 Dilawari, A. H. ; Szekely, J. , Metall. Trans. , 8B (1977) , 227. 36 Dilawari, A. H. ; Szekely, J. ibid. , 9B (1978) , 77. 37 Choudhary, M.; Szekely, J. , ibid, 11B (1980) , 439. 38 Zhmoidin, G. I. , Izv. Akad. Nauk. SSSR Met. , (1971) , №2, 29; (1972) , №4, 60. 39 Ling Yang; Derge, G. , Physical Chemistry of Process Metallurgy, Part Ⅰ, Intersciencc Publ. , New York, 1961, p. 503. 40 Edwards, J. B. ; Hucke, E. E. ; Martin, J. J. , Metall. Rev. 13 (1968) . №120. 1-12; 13-28. 41 Morgan, D. W. ; Kitchener, J. A. , Trans. Faraday Soc. , 50 (1954) , 51. 42 Darken, L. S. ; Gurry, R. W. , Physical Chemistry of Metals, McGraw-Hill, 1953, p. 484. 43 Duckworth, W. E. ; Hoyle, G. , Electroslag Refining, Chapman & Hall, London, 1969, pp. 40-44. 44 Mitchell, A. ; Joshi, S. , Metall. Trans. , 3 (1972) , 2306. 45 Hara, S. ; Ogino, K. , Int. Symp. on Metallurgical Slags, C. I. M. M. , Halifax, N. S. , August, 1980, Section 7. 46 Geiger, G. H. ; Poirier, D. R. , Transport Phenomena in Metallurgy, Addison-Wesley Publ. , 1973(中译本:俞景禄;魏季和译,冶金中的传热传质现象,冶金工业出版社,1981) ,p.18. 47 Joshi, S. , Ph. D. Thesis, University of British Columbia, 1971. 48 #12 49 Turkdogan, E. T. , BOF Steelmaking, Vol. Ⅱ (Theory), Chap. Ⅳ, Eds. Pehlke, R. D. ; Porter, W. F. ; et al. , AIME, New York, 1975, p. 45. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|