Please wait a minute...
金属学报  1986, Vol. 22 Issue (3): 33-37    
  论文 本期目录 | 过刊浏览 |
氢在Ta中的扩散
吕金钟;李文彬
北京钢铁学院;北京钢铁学院
DIFFUSION OF HYDROGEN IN Ta
by LU Jinzhong; LI Wenbin (Beijing University of Iron and Steer Technology)
引用本文:

吕金钟;李文彬. 氢在Ta中的扩散[J]. 金属学报, 1986, 22(3): 33-37.
, . DIFFUSION OF HYDROGEN IN Ta[J]. Acta Metall Sin, 1986, 22(3): 33-37.

全文: PDF(355 KB)  
摘要: 利用动态内耗方法测定了两种不同纯度Ta箔经电解充氢处理后在100—400K温度范围内的内耗值(Q~(-1)),并根据Gorsky原理计算了氢在Ta中的扩散系数。实验结果表明,在T>250K和T<180K的温度区间内氢的扩散系数D服从Arrhenius关系,同时计算了扩散常数D_0和激活能U。最后讨论了氢浓度和其它杂质对氢的扩散系数的影响。
Abstract:The long-range diffusion (Gorsky effect) of hydrogen in Ta has been studied as a function of temperature by means of the dynamical internal friction in the temperature range from 100—400 K. It is shown that the hydrogen diffusion coefficient, D, in 180 K>T and T>250K obeys the Arrhenius relation. The preexponential factor, D_0, and activation energy, U, have been calculated. The effects of hydrogen concentration and other impurities on the hydrogen diffusion coefficient were also discussed.
收稿日期: 1986-03-18     
1 Gorsky, W.S., Phys. Z., 8 (1935) , 457.
2 Cantelli, R.; Mazzolai, F.M.; Nuovo, M., J. Phys. (Paris), 32 (1971) , C2-59.
3 Bordoni, P.G., Nuovo Cimento, 4 (1947) , 177.
4 Cantelli, R,; Mazzolai, F.M.; Nuovo, M., Phys. Status Solidi, 34 (1969) , 597.
5 Qi, Zh.; Voelkl, J.; Wipf, H.; Alefeld, G., J, Phys. (Paris), 42 (1981) , C5-763.
6 Cannelli, G.; Cantelli, R., Hydrogen in Metals, V. 1, Proc. of 2nd Int. Congr., Paris, June, 1977, Pergamon Press, Oxford, New York, Paris.
7 Kokkinids, M., Diploma Thesis, Tech. Univ. Munchen, Germany, 1977.
8 Schaumann, G.; Voelkl, J.; Alefeld, G., Phys. Status Solidi, 42 (1970) , 401.
No related articles found!