铸铁石墨形态的转变及生长动力学 |
姚忻;丁少兰;吴学明;徐昭华;厉松春;王务献 |
上海交通大学;上海交通大学;上海交通大学;上海交通大学;上海交通大学;上海交通大学 |
|
TRANSITION OF GRAPHITE MORPHOLOGY IN CAST IRON AND ITS GROWTH KINETICS |
by YAO Xin; DING Shaolang; WU Xueming; XU Zhaohua; LI Songchun; WANG Wuxian (Shanghai Jiaotong University) |
引用本文:
姚忻;丁少兰;吴学明;徐昭华;厉松春;王务献. 铸铁石墨形态的转变及生长动力学[J]. 金属学报, 1986, 22(4): 80-82.
,
,
,
,
,
.
TRANSITION OF GRAPHITE MORPHOLOGY IN CAST IRON AND ITS GROWTH KINETICS[J]. Acta Metall Sin, 1986, 22(4): 80-82.