临界变形粗晶形成机理的探讨 |
吕炎;曲万贵;陈宗霖;穆安普 |
哈尔滨工业大学;哈尔滨工业大学;黎明机械公司;黎明机械公司 |
|
AN APPROACH TO MECHANISM OF COARSE GRAIN FORMATION AFTER CRITICAL DEFORMATION |
by Lü Yan; QU Wangui (Harbin Institute of Technology); CHEN Zonglin; MU Anpu (Liming Machinery Corp.; Shenyang)(Manuscript received 13 January; 1985; revised manuscript 4 February; 1986) |
引用本文:
吕炎;曲万贵;陈宗霖;穆安普. 临界变形粗晶形成机理的探讨[J]. 金属学报, 1986, 22(6): 41-146.
,
,
,
.
AN APPROACH TO MECHANISM OF COARSE GRAIN FORMATION AFTER CRITICAL DEFORMATION[J]. Acta Metall Sin, 1986, 22(6): 41-146.
1 Gorelik, S.S., Recrystallization in Metals and Alloys, MIR Publishers, Moscow 1981. p.227. 2 Burke, J. E., Shiau, Y.G., Trans. AIME, 175(1948) , 141. 3 吕炎;陈宗霖;穆安普;曲万贵等,高温合金文集,第五届全国高温合金年会,1984。 4 明旭光等,金属研究所,未公开发表资料,1983。 5 陈宗霖;吕炎;穆安普;曲万贵,金属科学与工艺,(1986) ,№4 |
|