| LD2合金过饱和固溶体的形变热处理 |
| 郑炀曾;王玉林;刘德富 |
| 东北重型机械学院;东北重型机械学院;东北重型机械学院 |
|
| THERMOMECHANICAL TREATMENT OF A SUPERSATURATED SOLID SOLUTION OF LD-2 ALUMINIUM ALLOY |
| ZHENG Yangzeng; WANG Yulin; LIU Defu (The Northeast Heavy Machinery Institute; Fulaerji; Heilongjiang) (Manuscript received 27 August; 1985; revised manuscript 17 April; 1986) |
引用本文:
郑炀曾;王玉林;刘德富. LD2合金过饱和固溶体的形变热处理[J]. 金属学报, 1987, 23(2): 118-239.
,
,
.
THERMOMECHANICAL TREATMENT OF A SUPERSATURATED SOLID SOLUTION OF LD-2 ALUMINIUM ALLOY[J]. Acta Metall Sin, 1987, 23(2): 118-239.
1 Blade J C, Bryant A J, Thomas A T. Met Technol 1976; 3: 380 2 邢广忠.硕士论文,东北重型机械学院,1982 3 Young C M, Sherby O D. In: Metal Forming: Interrelation Between Theory and Practice. New York: Plenum, 1971, 429 4 Gardner K J, Grimes R. Met Sci 1979; 13:216 5 王玉林,郑炀曾,刘德富.机械工程学报,1986;22:85 6 金子纯一.热处理,1981;21:331 |
|