Please wait a minute...
金属学报  1987, Vol. 23 Issue (3): 195-199    
  论文 本期目录 | 过刊浏览 |
Mg在一种镍基高温合金中的分布
马培立;庄景云;杨锦炎;高良
冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院
DISTRIBUTION OF Mg IN A Ni-BASE SUPERALLOY
MA Peili; ZHUANG Jingyun; YANG Jinyan; GAO Liang (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 25 October; 1985; revised manuscript 16 June; 1986)
引用本文:

马培立;庄景云;杨锦炎;高良. Mg在一种镍基高温合金中的分布[J]. 金属学报, 1987, 23(3): 195-199.
, , , . DISTRIBUTION OF Mg IN A Ni-BASE SUPERALLOY[J]. Acta Metall Sin, 1987, 23(3): 195-199.

全文: PDF(1420 KB)  
摘要: 研究Mg在一种镍基高温合金中的分布,Mg不仅富集于晶界,并且进入晶界二次碳化物和晶界及晶内γ′相中。
Abstract:The distribution of Mg in a Ni-base superalloy was observed to be not only enriched along the grain boundaries, but also entered into the secondary carbides of grain boundaries and γ'-phase, either along grain boundary or in the grains.
收稿日期: 1987-03-18     
1 #12
2 #12
3 可大年,仲增墉。金属学报,1983;19:A377-A384
4 Debarbodillo J J,郭文通译.高温合金:冶金学和生产,上海科学技术出版社,1980:58-67
5 Yamaguchi S, Kobayashi H, Matsumiya T, Hayami S. Met Technol, 1979; 6: 170-175
6 Guttmann M, Quantin B, Dumoulin Ph. Met Sci, 1983; 17(3) : 123-140
7 染野檀,安盛岩雄编,郑伟谋译。表面分析,科学出版社,1980:208
8 可大年,仲增墉.钢铁研究总院学报,1983;3(1) :73-80
9 藤田利夫,柴田诰司。日本金属学会会報,1977;16:231-238
No related articles found!