| 一水硬铝石型铝土矿溶出动力学的研究 |
| 顾松青;曹蓉江;陈新民 |
| 郑州轻金属研究所;北京有色金属研究总院;中南工业大学 |
|
| STUDY ON DIGESTION KINETICS OF DIASPORIC BAUXITE |
| by GU Songqing (Zhengzhou Light Metal Research Institute); CAO Rongjiang (Beijing General Research Institute of Nonferrous Metals); CHEN Xinmin (Central-South University of Technology) (Manuscript received 17 Octorber; 1985; revised manuscript 23 July; 1985) |
引用本文:
顾松青;曹蓉江;陈新民. 一水硬铝石型铝土矿溶出动力学的研究[J]. 金属学报, 1987, 23(6): 539-546.
,
,
.
STUDY ON DIGESTION KINETICS OF DIASPORIC BAUXITE[J]. Acta Metall Sin, 1987, 23(6): 539-546.