| Fe-C-N三元相图ε及γ′单相区界域 |
| 徐祖耀;李麟 |
| 上海交通大学材料科学与工程系;教授;山东工业大学 |
|
| PHASE BOUNDARIES OF SINGLE-PHASE ε-AND γ′-FIELDS IN Fe-C-N PHASE DIAGRAM |
| XU Zuyao (T. Y. Hsu);LI Lin Professor Department of Materials Science and Engtneering Shanghai Jiaotong University; Shandong polytechnic University |
引用本文:
徐祖耀;李麟. Fe-C-N三元相图ε及γ′单相区界域[J]. 金属学报, 1988, 24(1): 71-76.
,
.
PHASE BOUNDARIES OF SINGLE-PHASE ε-AND γ′-FIELDS IN Fe-C-N PHASE DIAGRAM[J]. Acta Metall Sin, 1988, 24(1): 71-76.
1 Naumann F K, Langenscheid G A. Arch Eisenhuettenwesen, 1965; 36: 677 2 Raghavan V. Trans Indian Inst Met, 1984; 37(4) : 293 3 Wells A, Bell T. Heat Treat Met, 1983; 10: 39 4 Elliott J F, Gleiser M, Ramarkrishna V. In: Elliott J F, Gleiser M eds., Thermochemistry for Steelmaking, London: Addison-Wesley Publishing Co. Inc. 1963: 405 5 Darken L S, Gurry R W. Physical Chemistry of Metals, McGraw-Hill, 1953: 379 6 Reed T B. Free Energy of Formation of Binary Compounds, MIT Press, 1971: 26 7 Dew-Hughes D, Kaufman L. CALPHAD. 1979; 3: 175 8 冯端,王业宁,邱第荣.金属物理,上册,科学出版社,1964:69 9 Kaufman L.CALPHAD,1978;2:295 10 徐祖耀.金属材料热力学,科学出版社,1981:254 11 范鸣玉,张莹.最优化技术基础,清华大学出版社,1982:164B |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|