| 熔盐钎剂与铝氧化膜的相互作用 |
| 张启运;刘淑祺;章于华 |
| 北京大学化学系;教授;北京大学;北京大学 |
|
| INTERACTION OF OXIDE FILM WITH MOLTEN FLUX DURING ALUMINUM BRAZING |
| ZHANG Qiyun;LIU Shuqi;ZHANG Yuhwa Dept. of Chemistry; Peking University |
引用本文:
张启运;刘淑祺;章于华. 熔盐钎剂与铝氧化膜的相互作用[J]. 金属学报, 1989, 25(2): 133-136.
,
,
.
INTERACTION OF OXIDE FILM WITH MOLTEN FLUX DURING ALUMINUM BRAZING[J]. Acta Metall Sin, 1989, 25(2): 133-136.
1 Jordan M F, Milner D R. J Inst Met, 1956--57: 85: 33 2 Terrill J R, Cochran C N, Stokes J J, Haupin W E. Weld J, 1971; 50: 833 3 #12 4 张启运,刘淑祺,郭海,简艾.金属学报,1985;21:B35 5 Yamaguchi S. Z Phys Chem, Leipzig, 1975; 256: 337 6 Stohr J, Johansson L I, Brennan S, Hecht M. Phys. Rev. B, 1980; 22: 4052 7 张启运,郑朝贵,刘淑祺.金属学报,1979;15:109" |
|