| 非晶态CoZr软磁薄膜的磁性 |
| 刘宜华;杨林倩 |
| 山东大学物理系;副教授;济南(250100);华侨大学 |
|
| MAGNETIC PROPERTIES OF AMORPHOUS CoZr SOFT MAGNETIC FILMS |
| LIU Yihua;YANG Linqian Shandong University; Jinan LIU Yihua; associate professor; Department of Physics; Shandong University; linan 250100 |
引用本文:
刘宜华;杨林倩. 非晶态CoZr软磁薄膜的磁性[J]. 金属学报, 1989, 25(6): 112-115.
,
.
MAGNETIC PROPERTIES OF AMORPHOUS CoZr SOFT MAGNETIC FILMS[J]. Acta Metall Sin, 1989, 25(6): 112-115.
1 Hayashi K, Hayakawa M, Ochiai Y, Matsuda H. Ishikawa W, Iwasaki Y, Aso K. J Appl Phys, 1987; 61: 2983 2 刘宜华,王德新,梅良谋.科学通报,1987;32(19) :1455 3 Liu Y H(刘宜华), Yang L Q(杨林倩). J Magn Magn Mater, 1988; 75: 263 4 Shimada Y, Kojima H. J Appl Phys, 1982; 53: 3156 5 Prutton M. Thin Ferromagnetic Films, London: Butterworths. 1964: 173 6 Kaul S N. Phys Rev, 1981; B24: 6550 7 Heiman N, Kazama N. Phys Rev, 1978; B17: 2215 |
|