| SmFe_(10-x)Co_xTi系列化合物的晶位及性质研究 |
| 张道元;熊曹水;孙天富;王征;黄美清 |
| 中国科学技术大学物理系;讲师;合肥(230026);中国科学技术大学;中国科学技术大学;中国科学技术大学;中国科学技术大学 |
|
| CRYSTALLOGRAPHIC SITES AND PROPERTIES OF SmFe_(10)-Co-xTi COMPOUNDS |
| ZHANG Daoyuan;XIONG Caoshui;SUN Tianfu;WANG Zheng;HUANG Meiqing University of Science and Technology of China; Hefei |
引用本文:
张道元;熊曹水;孙天富;王征;黄美清. SmFe_(10-x)Co_xTi系列化合物的晶位及性质研究[J]. 金属学报, 1991, 27(1): 148-150.
,
,
,
,
.
CRYSTALLOGRAPHIC SITES AND PROPERTIES OF SmFe_(10)-Co-xTi COMPOUNDS[J]. Acta Metall Sin, 1991, 27(1): 148-150.