| Gd-Pd-Pt三元系(Gd≤33at.-%)的室温和700℃等温截面 |
| 张康侯;陈藜莉 |
| 昆明贵金属研究所;昆明贵金属研究所 |
|
| ROOM TEMPERATURE AND 700℃ ISOTHERMAL SECTIONS OF Gd-Pd-Pt(Gd≤33 at. -%) PHASE DIAGRAM |
| ZHANG Kanghou;CHEN Lili Institute of Precious Metals; Kunming |
引用本文:
张康侯;陈藜莉. Gd-Pd-Pt三元系(Gd≤33at.-%)的室温和700℃等温截面[J]. 金属学报, 1991, 27(3): 147-149.
,
.
ROOM TEMPERATURE AND 700℃ ISOTHERMAL SECTIONS OF Gd-Pd-Pt(Gd≤33 at. -%) PHASE DIAGRAM[J]. Acta Metall Sin, 1991, 27(3): 147-149.