摘要: 研究了冷拉钢丝的变形及对强化的影响,结果表明:冷拉钢丝中的渗碳体片已成为易变形的塑性相,在Fe_3C/F界面上有许多“坎”(Ledge)存在,可发射位错,这可能是变形时造成Fe_3C/F界面有较高的位错密度原因之一;证实了位错可切过渗碳体片,必须考虑这一因素对强化的贡献。
关键词 冷拉钢丝位错胞    
Abstract:During cold-drawing of plain steel wires, the fine lamellar cementitealtered into a ductile phase with feasible deformability. A lot of ledges, which mayemit the dislocations, are found along the Fe_3C/Fe interface. This seems to be oneof the causes for formation of greater dislocation density along the Fe_3C/Fe inter-face during deformation. There was enough evidence to prove that the dislocationcut through Fe_3C. Therefore, it is necessary to consider its effect on strengthening.
Key wordsdeformation    strengthening    cold-drawn steel wire    dislocation cell    ledge    cementite
收稿日期: 1991-04-18     
1 Embury J D, Fisher R M. Acta Metall, 1966; 14: 147
2 Langford G, Cohen M. ASM Trans Q, 1969; 62: 623
3 Kelly A. Strengthening Methods in Crystals, Amsterdam: Elsevier, 1971: 331
4 Thompson A W. Metall Trans, 1977; 8A: 833
5 Nicholson R B. In: May M J ed, Effect of Second Phase Particle on the Mechanical Properties of Steel, ISI, London, 1971: 1, 61
6 黄孝瑛,郭薇,潘天喜,赵坚.金属学报,1987;23:A200
7 Li J C M, Chou Y T. Metall Trans, 1970; 1: 1145
8 Mintz B. Met Technol, 1984; 11: 265
9 Dollar M, Bernstein I M, Daeubler M, Thompson A W. Metall Trans, 1989; 20A: 447
10 Lindley T C, Oates G, Rochards C E. Acta Metall, 1970: 18: 1127
[1] 王俭秋;李劲;柯伟. 极化对A537钢低周腐蚀疲劳的近表面微观位错行为的影响[J]. 金属学报, 1996, 32(7): 730-734.
[2] 邹鸿承;戴蜀娟;钱志雄;李光霞. LY12CZ材料激光辐照延寿的微观研究及损伤演变[J]. 金属学报, 1989, 25(3): 51-56.