| 炉渣中SnS的挥发速率 |
| 华一新;刘纯鹏 |
| 昆明工学院;昆明工学院 |
|
| EVAPORATION RATE OF SnS FROM SLAGS |
| HUA Yixin;LIU Chunpeng Kunming Institute of Technology |
引用本文:
华一新;刘纯鹏. 炉渣中SnS的挥发速率[J]. 金属学报, 1992, 28(1): 57-61.
,
.
EVAPORATION RATE OF SnS FROM SLAGS[J]. Acta Metall Sin, 1992, 28(1): 57-61.
1 Daver T R A, Joffre J E. Trans Inst Min Metall, Sect C, 1973; 82: C145 2 Wright P A. Extractive Metallurgy of Tin, Amsterdam, Elsevier, 1966: 55 3 华一新,刘纯鹏.有色金属(季刊),1990;42(4) :49 4 Floyd J M. In: Cigan J M, Mackey T S, Okeefe T J eds, The Physical Chemistry of Tin Smelting, Lead-Zinc-Tin' 80, Proc Conf, Las Vegas, Nevade, February 24--28, 1980, AIME, 1980: 508 5 EL-Rahaiby S K, Rao Y K. Metall Trans, 1982; 13B: 633 6 Rankin W J. Metall Trans, 1986; 17B: 61 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|