Please wait a minute...
金属学报  1992, Vol. 28 Issue (11): 47-53    
  论文 本期目录 | 过刊浏览 |
偏心底吹熔池内三维流动的数值计算
李宝宽;赫冀成;陆钟武
东北工学院热能工程系;博士研究生沈阳(110006);东北工学院;东北工学院
MATHEMATICAL SIMULATION ON THREE DIMENSIONAL FLOW IN OFF-CENTER GAS STIRRED BATHS
LI Baokuan; HE Jicheng; LU Zhongwu (Northeast University of Technology; Shenyang)
引用本文:

李宝宽;赫冀成;陆钟武. 偏心底吹熔池内三维流动的数值计算[J]. 金属学报, 1992, 28(11): 47-53.
, , . MATHEMATICAL SIMULATION ON THREE DIMENSIONAL FLOW IN OFF-CENTER GAS STIRRED BATHS[J]. Acta Metall Sin, 1992, 28(11): 47-53.

全文: PDF(546 KB)  
摘要: 本文给出一种分析液态金属熔池内熔液三维流动的方法,按照保角变换理论,建立了适合计算偏心喷吹时熔池流场的非规范型正交曲线坐标系,用速度分量及压力作为流场的求解变量,发展了在非规范正交曲线系下求解三维、不可压缩、定常时均湍流Navier-Stokes方程,连续性方程,k—ε双方程湍流模型方程的数值计算方法,预示出了熔池及其模型内的流动状态,计算的熔池模型流场的的速度值同实验结果很接近。
关键词 : 偏心底吹熔池,  三维流动,  数值计算    
Abstract:This paper presents a method which can be used to predict threedimensional flow in gas stirred baths. A kind of general orthogonal curvilinear coordinates was established for calculating the flow in off-center gas stirred baths. Taking the velocity components and pressure as the solution variable, a method to produce the numerical solution of three-dimensional incompressible, steady, time averaged Navier -Stokes equation,continuity equation, k-εtwo equation turbulence model equations under general orthogonal curvilinear coordinates is develeped. The three-dimensional flow in bath can be clearly predicted by this calculation. The velocity vectors calculated for water model is approximately equal to the measured ones.
Key words: off-centred jetting    three dimensional flow    numerical calculation
收稿日期: 1992-11-18     
1 赫冀成.日本名古屋大学博士学位论文,1986
2 Asai S, Okamoto T, He Ji-Cheng, Muchi Ⅰ. Trans Iron Steel lnst Jpn, 1983; 23:43
3 Szekely J, Wang H Y, Kiser K M. Metall Trans, 1976; 7B:287
4 Grevet J H, Szekely J, El-Kaddah N. Int J Heat Mass Transfer, 1982; 25:487
5 李宝宽,赫冀成,陆钟武.第4届全国计算传热学术会议论文集,1991:312
6 李宝宽,赫冀成,陆钟武.中国工程热物理学会传热传质学术会议论文集,烟台,1991:119
7 李宝宽,东北工学院博士学位论文,1992
8 Mazumdar D. Metall Trans, 1989; 20B:967
9 Lnuder B E, Spalding D B. Comput Method Appl Mech Eng, 1974; 3:269
10 Castillejos A H, Brimacombe J K. Metall Trans, 1987; 18B:659
11 Joo S, Guthrie R I L, Kamal. G.Steelmaking Conference Proceeding, 1989. 517
[1] 邹德宁; 雷永平; 梁工英; 苏俊义 . 用数值计算技术和试错法确定金属材料表面对激光的吸收率[J]. 金属学报, 2001, 37(7): 737-740 .
[2] 孙阳; 冯乃祥; 崔建忠 . 186 kA大型预焙阳极铝电解槽磁场的三维数值计算[J]. 金属学报, 2001, 37(3): 332-336 .
[3] 罗键; 贾涛; 殷咸青; 贾昌申; 薛锦 . GTAW外加间歇交变纵向磁场的数值计算及其对焊接行为的影响[J]. 金属学报, 1999, 35(3): 330-333 .
[4] 赵连刚;朱苗勇;肖泽强. 柱坐标系下圆筒型反应器内三维湍流流动的数值模拟[J]. 金属学报, 1996, 32(1): 46-50.
[5] 朱苗勇;田郁夫;肖泽强. 吹氩精炼钢包内三维流动和混合现象的研究[J]. 金属学报, 1995, 31(20): 346-352.