| 非晶态Nd_4Fe_(77.5)(B_(1-x)C_x)_(18.5)合金的磁性和晶化 |
| 曹蕾;沈保根;杨林原;赵见高 |
| 中国科学院物理研究所磁学国家重点实验室;博士研究生;北京(100080);中国科学院物理研究所磁学国家重点实验室;中国科学院物理研究所磁学国家重点实验室;中国科学院物理研究所磁学国家重点实验室 |
|
| MAGNETIC PROPERTIES AND CRYSTALLIZATION OF AMORPHOUS Nd_4Fe_(77.5)(B_(1-x)C_x)_(18.5) ALLOYS |
| CAO Lei; SHEN Baogen; YANG Linyuan; ZHAO Jiangao (State Key Laboratory of Magnetism; Institute of Physics; Academia Sinica; Beijing) |
引用本文:
曹蕾;沈保根;杨林原;赵见高. 非晶态Nd_4Fe_(77.5)(B_(1-x)C_x)_(18.5)合金的磁性和晶化[J]. 金属学报, 1992, 28(11): 70-74.
,
,
,
.
MAGNETIC PROPERTIES AND CRYSTALLIZATION OF AMORPHOUS Nd_4Fe_(77.5)(B_(1-x)C_x)_(18.5) ALLOYS[J]. Acta Metall Sin, 1992, 28(11): 70-74.
1 Shen Baogen, Yang Linyuan, Zhang Junxian, Gu Benxi, Ning Taishan, Wo Feng, Zhao Jiangao, Guo Huiqun, Zhan Wenshan. Solid State Commun, 1990; 74:893 2 Shen Baogen, Zhang Junxian, Yang Linyuan, Wo Feng, Ning Taishan, Ji Songqian, Zhao Jiangao, Guo Huiqun, Zhan Wenshan. J Magn Magn Mater, 1990; 89:195 3 Shen Baogen, Yang Linyuan, Zhang Junxian, Wo Feng, Ning Taishan, Zhao Jiangao, Guo Huiqun, Zhan Wenshan. J Magn Magn Mater. 1991; 96:335 4 Zhang Junxian, Shen Baogen, Yang Linyuan, Zhan Wenshan. Phys Status Solidi, 1991; 12a:541 5 杨红缨,沈保根,杨林原,郭慧群.金属学报,1992;28:B159 6 Zhang JunXian, Shen Baogen, Yang Linyuan, Zhan Wenshan. Phys Status Solidi, 1990; 122a:651 7 Shen Baogen, Zhang Junxian, Yang Linyuan, Guo Huiqun, Zhao Jiangao. Mater Sci Eng. 1991; A133:162 8 Luborsky F E, Becker J J, Walter J L, Martin D L. IEEE Trans Magn. 1980; MAG-16:521< |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|