| 原位生长纤维状多型体AlN复合陶瓷材料的显微结构与力学性能 |
| 李宗怀;陈声崎;周延春;夏非 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;研究员沈阳110015 |
|
| MICROSTRUCTURE AND MECHANICAL PROPERTIES OF IN-SITU FORMATION FIBROUS POLYTYPE AIN COMPOSITE MATERIAL |
| LI Zonghuai; CHEN Shengqi; ZHOU Yanchun; XIA Fei (Institute of Metal Research; Academia Sinica; Shenyang) |
引用本文:
李宗怀;陈声崎;周延春;夏非. 原位生长纤维状多型体AlN复合陶瓷材料的显微结构与力学性能[J]. 金属学报, 1992, 28(7): 90-94.
,
,
,
.
MICROSTRUCTURE AND MECHANICAL PROPERTIES OF IN-SITU FORMATION FIBROUS POLYTYPE AIN COMPOSITE MATERIAL[J]. Acta Metall Sin, 1992, 28(7): 90-94.
1 Shalek P D, Petrovic J J, Hurley G F, Gac F D. Am Ceram Soc Bull, 1986; 65: 351 2 Rafaniello W, Cho K, Virkar A V. J Mater Sci, 1981; 16: 3479 3 Tronleli M, Kolar D. In: Popper P ed., Special ceramics 6, Proc 6th Symposium on Special Ceramics, Stoke-on-Trent, July 9-11, 1974, Manchester, 1975; 6: 39 4 Evans A G, Char E A. J Am Ceram Soc, 1976; 59: 371 5 Hever A H, Fryburg G A, Ogbuji L U, Mitchell T E, Shinozaki S. J Am Ceram Soc, 1978; 61: 409 6 Jack K H, In: Riley F L ed., Nitrogen Ceramics, Noordhooff, Leyden, 1977: 109 7 Chase A B, Osmer J A. J Cryst Growth, 1972; 15: 249 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|