| DD3单晶镍基合金蠕变-疲劳及寿命预测 |
| 苏翰生;吴仲棠 |
| 北京航空材料研究所;高级工程师;北京(100095)北京81号信箱23号分箱;北京航空材料研究所 |
|
| CREEP-FATIGUE BEHAVIOUR OF A Ni-BASE SINGLE CRYSTAL ALLOY DD3 AND ITS LIFE PREDICTION |
| SU Hansheng;WU Zhongtang Beijing Institute of Aeronautical Materials |
引用本文:
苏翰生;吴仲棠. DD3单晶镍基合金蠕变-疲劳及寿命预测[J]. 金属学报, 1993, 29(1): 25-32.
,
.
CREEP-FATIGUE BEHAVIOUR OF A Ni-BASE SINGLE CRYSTAL ALLOY DD3 AND ITS LIFE PREDICTION[J]. Acta Metall Sin, 1993, 29(1): 25-32.
1 Miner R V, Gayda J, Hebsur M G. ASTM STP 942. 1988; 371 2 Gabb T P, Welsch G, Miner R V, Gayda J. Mater Sci Eng. 1989: A108: 189 3 Duan Z, He J, Ning Y, Dong Z. ASTM STP 942, 1988: 1133 4 Hoffelner W, Melton K N, Wuethrich C. Fatigue Eng Mater Struct, 1983; 6: 77 5 Draprel J M. AD/A059900, 1978, Al--9----Al--43 |
|