| 碳纤维表面气相生长碳晶须 |
| 孙守金;魏永良;刘敏;李敏君 |
| 中国科学院金属研究所;助理研究员;沈阳110015;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| CHEMICAL VAPOUR GROWTH OF CARBON WHISKERS ON CARBON FIBRE |
| SUN Shoujin;WEI Yongliang;LIU Min;LI Minjun Institute of Metal Research Academia Sinica; Shenyang research associate;Institute of Metal Research;Academia Sinica;Shenyang 110015 |
引用本文:
孙守金;魏永良;刘敏;李敏君. 碳纤维表面气相生长碳晶须[J]. 金属学报, 1993, 29(4): 62-67.
,
,
,
.
CHEMICAL VAPOUR GROWTH OF CARBON WHISKERS ON CARBON FIBRE[J]. Acta Metall Sin, 1993, 29(4): 62-67.
1 Ko F K. Am Ceram Soc Bull, 1989: 68: 401 2 Bahl O P, Mathur R B. Polym Eng Sci, 1984; 24: 455 3 Fitzer E, Geigl K-H, Huttner W, Weiss R. Carbon, 1980; 18: 389 4 张志谦,张德庆、魏月贞、宇航材料工艺,1991;(2) :41 5 Jones C, Sammann E. Proceedings of the American Society for Composites. 14th Technical Conference. Lancaster, USA: Technomic, 1989: 387 6 Tibbetts G G. In: Figueiredo J L, Bernardo C A, Baker R T K, Huttinger K J eds., Carbon Fibers Filaments and Composites. Dordrecht: Kluwer Academic, 1989: 147> |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|