低碳低钒钢中细小沉淀对微裂纹扩展的影响
王四清;陈梦谪;柯俊
冶金工业部长沙矿冶研究院材料2室;工程师;长沙410012;北京科技大学;北京科技大学
EFFECT OF FINE PRECIPITATES ON PROPAGATION OF MICRO-CRACKS IN LOW CARBON LOW VANADIUM STEEL
CHEN Mengzhe;KE Jun University of Science and Technology BeijingWANG Siqing;engineer;Changsha Institute of Mining and Metallrugy;Ministry of Metallurgical Industry.Changsha 410012
引用本文:

王四清;陈梦谪;柯俊. 低碳低钒钢中细小沉淀对微裂纹扩展的影响[J]. 金属学报, 1993, 29(5): 23-27.
, , . EFFECT OF FINE PRECIPITATES ON PROPAGATION OF MICRO-CRACKS IN LOW CARBON LOW VANADIUM STEEL[J]. Acta Metall Sin, 1993, 29(5): 23-27.

全文: PDF(1753 KB)  
摘要: 在透射电镜下原位观察低碳低钒钢中细小第?相沉淀粒子(平均直径86nm)对微裂纹的形成与扩展的影响.结果表明,细小的第二相沉淀粒子(VC)群将通过阻碍裂纹尖端前方区域的位错运动,减缓局部区域薄化过程,阻碍微裂纹的形成和扩展,从而对微裂纹的扩展路径起一定的控制作用,而单个细小的第二相沉淀粒子对这种作用的影响将不大
关键词 : 第二相沉淀粒子,  微裂纹扩展,  钒钢    
Abstract:The fine second phase particles, average size about 86 nm, precipitating inferrite matrix of low carbon low vanadium steel will hinder the movement of dislocations infront of crack-tip, retard the thinning process in local area, and then proceed to impede theinitiation and propagation of micro-cracks. The propagating path of micro-cracks is control-led partly by the distribution of precipitates, a single particle has the action aforementionedweakly.
Key words: second phase    precipitation    micro-crack    dislocation    V steel
收稿日期: 1993-05-18     
基金资助:国家自然科学基金
1 Gladman T. Effect of Second-Phase Particles on the Mechanical Properties of Steel. London: The Iron and Steel Institute, 1971: 68
2 Fisher J R. Gurland J. Met Sci, 1981; 15: 185
3 Inoue T, Kinoshita S. Trans Iron Steel Inst Jpn. 1977: 17: 523
4 Ritchie R O. Thompson A W. Metall Trans, 1986; 16A: 233
5 Chan I Y. Wilsdorf H G F. Acta Metall, 1981; 29: 1221
6 Benson J P, Edmonds D V. In: Taplin DMR ed., Fracture 1977. Vol. Ⅱ, Proc 4th Int Conf on Fracture, New York: Pergamon, 1978: 65
7 张以增.戴蜀娟.邹鸿承,苗丕峰.金属学报,1987;23:A403
8 Jagannadham K, Wilsdorf H G F. Mater Sci Eng, 1986: A81: 273
9 Ohr S M. Mater Sci Eng, 1985; A72: 1=
No related articles found!