Please wait a minute...
金属学报  1993, Vol. 29 Issue (8): 55-60    
  论文 本期目录 | 过刊浏览 |
CO还原CaO—SiO_2—Fe_tO三元渣系的研究
杨学民;王大光;宣德茂
助理研究员;北京(100080);中国科学院化工冶金研究所二室;中国科学院化工冶金研究所;中国科学院化工冶金研究所
REDUCTION OF CaO-SiO2-Fe_tO TERNARY SLAG BY CO
YANG Xuemin;WANG Daguang;XUAN Demao Institute of Chemical Metallurgy; Academia Sinica; BeijingDepartment No.2;Institute of Chemical Metallurgy;Academia Sinica; Beijing 100080
引用本文:

杨学民;王大光;宣德茂. CO还原CaO—SiO_2—Fe_tO三元渣系的研究[J]. 金属学报, 1993, 29(8): 55-60.
, , . REDUCTION OF CaO-SiO2-Fe_tO TERNARY SLAG BY CO[J]. Acta Metall Sin, 1993, 29(8): 55-60.

全文: PDF(430 KB)  
摘要: 在1723K进行了CO还原CaO—SiO_2-Fe_(t)O三元渣系的研究根据CO_2红外分析仪测定的出口气体中的CO_2浓度变化,计算了炉渣的表观还原速度常数K_(a)结果表明,K_(a)随炉渣中Fe_1O量增加呈抛物线变化;当炉渣碱度R<1.0,Fe_(t)O为50%和R为1.5,Fe_(t)O为70%时,K_(a)分别出现最小值用炉渣规则溶液模型可计算1723K时的CaO-SiO_2-Fe_tO三元渣系的Fe_1O活度值a_(Fe_1O)。
关键词 : CaO—SiO_2-Fe_1O三元渣系,  CO气体还原,  Fe_1O活度,  规则溶液模型    
Abstract:Apparent reduction rate constant, K_a, was determined by measuringCO_2 evolution with an infrared gas analyser. The relationship between K_a and Fe_tO in slagwas found to be parabolic. K_a approaches to the minimum when either the slag basicity,R<1.0 or=1.5 and Fe_tO content 50% or 70%,respectively. The activities of Fe_tO in CaO-SiO_2- Fe_tO ternary slag system at 1723 K may be calculated by using regular solution model.
Key words: CaO-SiO_2-Fe_tO system    reduction    activity    reduction rate
收稿日期: 1993-08-18     
基金资助:中国科学院;;国家自然科学基金
1 Nagasaka T, Iguchi Y, Ban--Ya S. Fifth International Iron and Steel Congress, April 6--9,1986; Washington,D.C.U.S.A.
2 Fine H A,Meyer D,Janke D,Engel H-J. Ironmaking and Steelmaking. 1985; 12(4) : 157
3 杨学民,王大光,宣德茂,唐武成.第八届全国冶金物理化学学术研讨会论文集,苏州,1992:153
4 杨学民,王大光,宣德茂,刘天中.冶金学科青年学术交流会论文集,沈阳,1991
5 杨学民,王大光,宣德茂.化工冶金,1993;14:139
6 杨学民,王大光,宣德茂.化工冶金,待发表
7 陈稼祥 编著.炼钢常用图表手册.北京:冶金工业出版社,1984:150,635
8 陈襄武.钢铁冶金物理化学.北京:冶金工业出版社,1990:51
9 Lumsden J. Physical Chemistry of Process Metallurgy, Part Ⅰ. New York: Interscience, 1961: 165
10 Turkdogan E T. Physicochemsitry of Molten Slags and Glasses, London, The Metal Socity 1983
11 万谷志郎,日野光兀.铁钢,1987;73:476H
[1] 杨学民;郭占成;于宪溥;艾菁;王大光. CO还原CaO-SiO_2-Al_2O_3-Fe_tO渣系研究[J]. 金属学报, 1994, 30(23): 491-498.