加弧辉光放电等离子表面合金化
潘俊德;范本惠;李成明;贺琦;郑维能;徐重
太原工业大学;太原工业大学;太原工业大学;太原工业大学;太原工业大学;太原工业大学
SURFACE ALLOYING BY GLOW-DISCHARGE PLASMA WITH ARC SOURCE
PAN Junde;FAN Benhui;LI Chengming;HE Qi;ZHENG Weineng;XU Zhong Taiyuan University of Technology
引用本文:

潘俊德;范本惠;李成明;贺琦;郑维能;徐重. 加弧辉光放电等离子表面合金化[J]. 金属学报, 1993, 29(9): 88-91.
, , , , , . SURFACE ALLOYING BY GLOW-DISCHARGE PLASMA WITH ARC SOURCE[J]. Acta Metall Sin, 1993, 29(9): 88-91.

全文: PDF(651 KB)  
摘要: 介绍了加弧辉光离子渗金属装置及基本原理在辉光离子渗金属装置中,引入冷阴极电弧源,实现了快速渗金属,已成功地在普通碳钢表面渗入Ti,Al及Cr—Ni等合金元素,同时分析了10钢渗Ti处理后的渗层组织特征、成分分布、相组成及工艺参数对渗层的影响
关键词 : 辉光放电,  弧光放电,  表面合金化,  冷阴极电弧源    
Abstract:Investigation was carried out of titanizing the plain steel by technique ofglow-discharge plasma with arc source. Microstructure, Ti distribution and phases occurredin the infiltration layer and their related processing parameters were examined and discussed.
Key words: glow-discharge    arc-discharge    surface alloying    cold cathode arc source
收稿日期: 1993-09-18     
基金资助:山西省自然科学基金及留学生资助项目
1 潘俊德,范本惠,徐重,李成明,韩晋宏,郑维能.CN Pat,90103841. 5,1990
2 Xu Zhong.USA Pat,4520268,1985
3 徐重,王振民,古凤英,范本惠,肖丽华,赵晋香.金属热处理学报,1982;(1) :71
4 张石权.真空,1988;(1) :7
5 王福珍,闻立时.表面沉积技术.北京:机械工业出版社,1989:31
[1] 周霞; 王越; 周继扬; 曲国辉; 鲍志勇 . WC颗粒增强铜基合金覆层用钎料的研究[J]. 金属学报, 2007, 43(4): 433-438 .
[2] 陈涛; 常海威; 雷明凯 . Al离子高温注入Fe靶的表面合金化研究[J]. 金属学报, 2005, 41(4): 417-420 .
[3] 王华明; 于利根; 李晓轩; 蒋平 . MC碳化物准快速凝固形态与生长机制研究[J]. 金属学报, 1999, 35(12): 1246-1248 .
[4] 何秀丽;王华明;郑启光;许德胜. TiAl金属间化合物碳元素激光表面合金化[J]. 金属学报, 1998, 34(9): 983-986.
[5] 贺琦;边洁;郑维能;潘俊德;范本惠. 加弧辉光离子Ni-Cr共渗层的显微组织[J]. 金属学报, 1997, 33(4): 406-412.
[6] 于力;金柱京;黄燕清;朱天锦;吉川一功. Co对弧光放电离子镀WC-Co膜生长的影响[J]. 金属学报, 1994, 30(17): 229-232.
[7] 任建世;张功杼;王桢枢;刘根;刘圣麟. 辉光放电灯中二元合金溅射率与化学组成的关系[J]. 金属学报, 1992, 28(5): 85-89.
[8] 王正;张永升. Ni-P化学镀层对304钢应力腐蚀开裂的影响[J]. 金属学报, 1991, 27(2): 129-134.
[9] 任建世;赵惠林;张功杼. 镍基合金辉光放电阴极溅射表面形貌[J]. 金属学报, 1989, 25(4): 148-150.