| 形变温度对Ti_3Al基合金α_2相滑移系的影响 |
| 孙福生;高文;曹春晓 |
| 北京航空材料研究所 |
|
| INFLUENCE OF DEFORMATION TEMPERATURE ON α_2-PHASE SLIP SYSTEMS OF A Ti_3Al ALLOY |
| SUN Fusheng;GAO Wen;CAO Chunxiao(Institute of Aeronautical Materials; Beijing)(Manuscript received 31 August; 1993; in revised form 22 November; 1993) |
引用本文:
孙福生;高文;曹春晓. 形变温度对Ti_3Al基合金α_2相滑移系的影响[J]. 金属学报, 1994, 30(11): 507-514.
,
,
.
INFLUENCE OF DEFORMATION TEMPERATURE ON α_2-PHASE SLIP SYSTEMS OF A Ti_3Al ALLOY[J]. Acta Metall Sin, 1994, 30(11): 507-514.
| 1BlackburnMJ,SmithMP.AirForceTechRepAFWAL-TR-81-4046,19812LipsittHA.In:C.C.Koch,LiuCT.StoloffNSeds.,HighTemperatureOrderedIntermetallicAl-loys,Pittsburgh,PA:MRS,1985:3513YongWJS.MetallTrans,1982:18A:3244CourtSA,LorettoMH,FraserHL.ScrMetall,1987;21:9975ThomasM,VasselA,VeyssiereP.ScrMetall,1987;21:5016WilliamsJC.In:WilliamsJC,BeloyAFeds.,TitaniumandTitaniumAlloys,Vol.2,NewYork:PlenumPress,1982:14777 SastrySM,LipsittHA.MetallTrans,1977;8A:15438BanerjeeD,GogiaAK.NandyTK,MetallTrans,1990;21A:6279孙福生,李成功,曹春晓.材料工程,1992;7-9:3210FriedalJ.Dislocation.PergamonPress,1964p |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|