金属学报  1994, Vol. 30 Issue (22): 439-443    
  论文 本期目录 | 过刊浏览 |
锂盐碳阳极的可湿性与临界电流密度研究
邱竹贤;姚广春;于亚鑫;张中林
东北大学
WETTABILITY AND CRITICAL CURRENT DENSITY OF LITHIUM SALT-CONTAINING CARBON ANODE
QIU Zliuxian;YAO Guangchun;YU Yaxin;ZHANG Zhonglin(Northeastern University; Shenyang)
引用本文:

邱竹贤;姚广春;于亚鑫;张中林. 锂盐碳阳极的可湿性与临界电流密度研究[J]. 金属学报, 1994, 30(22): 439-443.
, , , . WETTABILITY AND CRITICAL CURRENT DENSITY OF LITHIUM SALT-CONTAINING CARBON ANODE[J]. Acta Metall Sin, 1994, 30(22): 439-443.

全文: PDF(300 KB)  
摘要: 含有锂盐的碳阳极的可湿性和发生阳极效应的临界电流密度值明显提高,可以防范阳极效应的发生,文中讨论了锂盐的作用机理。
关键词 : 锂盐碳阳极,  可湿性,  临界电流密度    
Abstract:The lithium salt-containing carbon anode is with better wettability and higher critical current density than the ordinary carbon anode.The occurrence of anode effect in aluminium electrolysis may be decreased by using this type of carbon anode in industrial cells.The mechanism of inhibiting anode effect is explained.
Key words: lithium salt-containing carbon anode    wettability    critical current density
    
基金资助:国家自然科学基金
QiuZhuxian,WeiQingbin,YaoKwantsung,Aluminium,1983;9:6702HarkerH.ProceedingsoftheFourthConferenceonCarbon.England,1960:1253FrankWB,HaupinWE,DawlessRK.Ullmann'sEncyclopediaofIndustrialChemistry,1985;Al:4594PiontelliR.J ElectrochemSoc,1956;103:7055WatanebeN,ChongYB,AritsukaM,ProceedingsoftheFourthJapan-ChinaBilateralConferenceonMoltenSalts,Japan,1992:1116TojoT,HiraiwaJ,WatanabeN.ProceedingsofthefouthJapan-ChinaBilateralConferenceonMoltenSalts,Japan,1992:1157LiuYexiang,XiaoHM,ChenXG.LightMetals,1991:48