| 考虑热不协调性的镍基单晶合金细观力学分析 |
| 岳珠峰;郑长卿 |
| 西北工业大学 |
|
| MICRO-MECHANICAL ANALYSIS OF THERMAL MISFIT OF SINGLE CRYSTAL Ni-BASE SUPERALLOY |
| YUE Zhufeng;ZHENG Changqing(Northwestern Polytechnical University;Xi'an)(Manuscript received 2 April;1993;in revised form 24 September;1993) |
引用本文:
岳珠峰;郑长卿. 考虑热不协调性的镍基单晶合金细观力学分析[J]. 金属学报, 1994, 30(3): 124-132.
,
.
MICRO-MECHANICAL ANALYSIS OF THERMAL MISFIT OF SINGLE CRYSTAL Ni-BASE SUPERALLOY[J]. Acta Metall Sin, 1994, 30(3): 124-132.
| 1LallC,ChinS,PopeDP.MetallTrans,1979;10A:1323-13322PaidarV,Pope,DP,VitekV,ActaMetall,1984;32:435-4483MullerL,GlatzelU,Feller-KniepmeierM.ActaMetallMater,1992;40:1321-13274MullerL,LinkT,Feller-KniepmeierM.ScrMetallMater,1992;26:1297-13025GaydaJ,MackayRA.ScrMetall.1989;23:1835-18386GlatzelU,Feller-KniepmeierM.ScrMetall,1989;23:1839-18447DandekarDP,MartinAG.JMaterSci.1990;25:3321-33268ButtnerN,FusenigKD,NembachE.ActaMetalL1987;35:845-8549NembachN,SchanzerS,SchrorerW,TrinckanfK.Acta MetalL,1983;36:1471-147910Schanzers,NembachE.ActaMetall,Mater,1992;40:803-81311ReppichB,ScheppP,WehnerG.ActaMetall,1982;30:95-10412ShahBD,DuhlDN.In:GellM,KovtovichCS,BricknellRH,KentWB,RadavichKE,eds,Superalloys1984,Proc.5thInt.Symp.onSuperalloys,AIME,Warrendale,PA,1984:105-11413岳珠峰,郑长卿.航空学报,1993;14:A556-55914TienJK,CopleySM.MetallTransA,1971;2:543-55315冯端.结构与缺陷.北京:科学出版社,1988:525-52716BrownAM,AshbyMF.ActaMetall,1980;28:1085-110117StrangmanTE,HeathB,FujiiM.Low-CostSingleCrystalTurbineBlades,NASACR-168218,1983 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|