| 静压下扩散反应形成块状Al-Fe(Mo,Si,B)纳米合金 |
| 姚斌;丁炳哲;李冬剑;王爱民;胡壮麒 |
| 中国科学院金属研究所快速凝固非平衡合金国家重点实验室;四平师范学院 |
|
| PREPARATION OF BULK Al-Fe(MO, Si, B)NANOSTRUCTURED ALLOY BY DIFFUSION REACTION UNDER HIGH PRESSURE |
| YAO Bin; (Institute of Metal Research; Chinese A cademy of Sciences; Shenyang 110015)DING Bingzhe; LI Dongjian; WANG Aimin; HU Zhuangqi (State Key Laberatory for RSA; Institute of Metal Research; Chinese Acadeimy of Sciences; Shenyang 110015)(Siping Normal College; Siping 136000) |
引用本文:
姚斌;丁炳哲;李冬剑;王爱民;胡壮麒. 静压下扩散反应形成块状Al-Fe(Mo,Si,B)纳米合金[J]. 金属学报, 1995, 31(17): 220-225.
,
,
,
,
.
PREPARATION OF BULK Al-Fe(MO, Si, B)NANOSTRUCTURED ALLOY BY DIFFUSION REACTION UNDER HIGH PRESSURE[J]. Acta Metall Sin, 1995, 31(17): 220-225.
| 1BirringerR,HerrU,GleiterH.SupplTransJpnInstMet.1986;27:432QiXY,WuWJ,ChengLF.NanostructMater,1993;2(1):993HahnH,LogasJ,AverbackRS.JMalerRes,1990;5(3):6094UhlmannDR,HaysJF,TurnbullD.PhysChemGlasses.,1966;7(5):1595StrozkajaGG.Ph.Dthesis,HighPressurePhysicsInstitute,Moscow,19886XuY,HuangX,WangWK.ApplPhysLett,1990;56:19577LarchevVT,MelnikNN,PopovaSV,StrotskayaGG,TalenskijON.ProcLebedev,PhysInstitute,1985;1:7(inRussian)8姚斌,张强,苏文辉.高压物理学报,1990;4(1):509LiDJ,DingBZ,YaoB,HuZQ.NanostructMuter,1994;4:32310汪复兴主编.金属物理.北京:机械工业出版社,1981:167 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|