| 几种铝化合物的热力学性质 |
| 陈启元;曾文明;张平民;顾松青;杨冠群;周辉放;尹中林 |
| 长沙中南工业大学;郑州轻金属研究院;中南工业大学化学系 |
|
| THERMODYNAMIC PROPERTIES OF SOME ALUMINUM COMPOUNDS |
| CHEN Qiyuan; ZENG Wenming; ZHANG Pingmin (Central-South University of Technology; Changsha 410083)GU Songqing; YANG Guanqun; ZHOU Huifang; YIN Zhonglin (Zhengzhou Research institute of Light Metals; Zhengzhou 450041) (Manuscript received 1995-02-23; in revised form 1995-06-29) |
引用本文:
陈启元;曾文明;张平民;顾松青;杨冠群;周辉放;尹中林. 几种铝化合物的热力学性质[J]. 金属学报, 1996, 32(1): 6-14.
,
,
,
,
,
,
.
THERMODYNAMIC PROPERTIES OF SOME ALUMINUM COMPOUNDS[J]. Acta Metall Sin, 1996, 32(1): 6-14.
| 1FurukawaGT,DouglasTB,McCoskeyRE,GinningsDC.JResNatBurStand,1956;57:672EdwardsJW,KingtonGL.TransFaradySoc,1962;58:13133ChekhovskoiVYa.HighTemp,USSR,1964;2:2644BuycoEH.Proceedingsofthe4thsymposiumonThermophysicalProperties,NewYork:ASME,1968:1615ViswanathanR.JApplPhys,1975;46:40866ChangSS.Proceedingsofthe7thSymposiumonThermophysicalProperties,NewYork:ASME,1977:837DitmarsDA,IshiharaS,ChangSS,BernsteinG,WestED.JResNatBurStand,1982;87:1598CastanetR.HighTempHighPressures,1984;16:4499ParksGS,KelleyKK.JPhysChem,1926;30:4710ShomateCH,NaylorBF.JAmChemSoc,1945;67:7211DitmarsDA,DouglasTB.JResNatBurStand,1971;75:40112ShmidNE,SokolovVA.RussJInorgChem,1960;5:79713RomanovskiiVA,TarasovVV.SovPhysSolidState,1960;2:117614PalkinVA,KuzminaNN,ChernyaevII.RussJInorgChem,1965;10:2315SchauerA.CanJPhys,1965;43:52316MartinDL,SnowdonRL.CanJPhys,1966;44:144917GopalaRaoRV,GunjikarVG,SankarSG,BiswasAB.IndianJPureApplChem,1967;5:9918GronvoldF.ActaChemScand,1967;21:169519MartinDL,SnowdonRL.RevSciInstrum,1970;41:186920OnoderaN,KimotoA,SakiyamaM,SekiS.BullChemSocJpn,1971;44:146321GronvoldF.ActaChemScand.1972;26:221622TakahashiY,YokokawaH,KadokuraH,SekineY,MukaiboT.JChemThermodyn,1979;11:37923WalkerBE,GrandJA,MillerRR.JPhysChem,1956;60:23124FrederiksonDR,ChasanovMG.JChemThermodyn,1970;2:62325MurabayashiM,TakahashiY,MukaiboT.JNuclSciTech,1970;7:31226MacLeodAC.JChemThermodyn,1972;4:69927FomichevEN,BondarenkoVP,KandybaVV.HighTempHighPressures,1973;5:128EfremovaRI,MatizenEV.HighTempHighPressures,1976;8:39729ShmidtNE,MaksimovDN,RussJPhysChem,1979;53:108430ShmidtNE.RussJInorgChem,1966:11:24131FerrierA,OletteM.CRAcadSci.1962;254:429332ProphetH,StullDR.JChemEngData,1963;8:7833ParksGS,KelleyKK.BurMinesBull,1941;434:11534CoxJD,WagmanDD,MedvedevVA.CODATAKeyValuesforThermodynamics.NewYork:HemispherePublishingCorporation,1989:2135FugateRQ,SwensonCA,JApplPhys,1969;40:303436AppsJA,NeilJM.ACSSympSeries416.WashingtonDC,1990:41537RobieRA,HemingwayBS,FisherJR.USGeolSurvBull,1979:145238SnyderPE,SeltzH.JAmChemSoc,1945;67:68339HolleyCE,HuberEJJr.JAmChemSoc,1951;73:557740SchneiderA,GattowG.ZAnorgAllgemchem,1954;277:4141MahAD,JPhysChem,1957;61:157242ZenkovID.RussJPhysChem,1981;55:169843ChaseMW,CurnuttJL,McDonaldRA,SyverudAN.JPhysChemRefData,1978;7:793,83844HemingwayBS,RobieRA,KittrickJA.GeochimCosmochimActa,1978;42:153345MarchidanDI,PandeleL,NicolescuA.RevRoumChim,1972;17:149346ChenQ,ZengW,ChenX,GuS,YangG,ZhouH,YinZ.ThermochimActa,1995;253:3347BorerWJ,GunthardHH.HelvChimActa,1970;53:104348YokokawaT,KleppaOJ.JPhysChem,1964;68:324649ShomateCH,CookOA,AmChemSocJ,1946;68:214050HemingwayBS,RobieRA,FisherJR,WilsonWH.JResUSGeoSurv,1977;5:79751ChenQ,ZengW.GeochimCosmochimActa,1996,tobepublished52HemingwayBS,RobieRA.JResUSGeolSurv,1977;5:41353GrossP,ChristieJ,HaymanC.FulmerResInstRept6,1970,PG//JMN//R:2454BaranyR,KelleyKK.USBurMinesReptInv5825,1961;1355CoughlinJP.JPysChem,1958;62:41956ZengW,ChenQ,ChenX.GeochimCosmochimActa,1994;58:351157PalmerDA,WesolowskiDJ.GeochimCosmochimActa,1992;56:109358ChenQ,ZengW.JCentSouthUnivTech(EngEdit),1995;2:759HemingwayBS,RobieRA,AppsJA.AmMineralogist,1991;76:44560RusselAS,EdwardsJD,TaylorCS.JMetals,AIME,1955;203:112361KuyunkoNS,MalininSD,KhodakovskiyIL,GeochemInt,1983;20:7662KostomaroffV,ReyM.SilicatesIndustry,1963;28:963AppsJA,NeilJM,JunC-H,LawrenceBerkeleyLaboratoryRept21482,198864ZengW,ChenQ,ChenX.JChemThermodyn,1994;26:20565KingEC,BaranyR,WellerWW,PankratzLB.USBurMinesReptInv6962,196766MukaiboT,TakahashiY,YamadaK.Proc1stIntConfCalorThermodyn,Warsaw;1969:35767PerkinsD,EsseneEJr,WAllV.AmMineralogist,1979;64:108068FyfeWS,HollanderMA.AmJSci,1964;262:70969HassH.AmMineralogist,1972;57:137570SabatierG.BullSocFrMineralCrystallogr,1954;77:107771ZengW,ChenQ,GuS,YangG,ZhouH,YinZ.JChemThermodyn,1995;27:44372周红,曾文明,陈启元.中国有色金属学报,1993;3:4073PeryeaFJ,KittrickJA.ClaysClayMinerals,1988;36:391. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|