| Fe_(73.5)Cu_(1.0)Mo_(3.0)Si_(13.5)B_(9.0)纳米软磁合金的结构与磁性 |
| 纪松;杨国斌;王润 |
| 中国兵器工业第五二研究所宁波分所;北京科技大学 |
|
| MICROSTRUCTURE AND MAGNETIC PROPERTIES OF NANOSTRUCTURED SOFT MAGNETIC ALLOY Fe_(73.5) Cu_(1 .0)Mo_(3.0)Si_(13.5)B_(9.0) |
| JI Song (Research Institute No.52 of China Ordnance industry; Ningbo Branch;Ningbo 315040);YANG Guobin; WANG Run (University of Science and Technology Beijing; Beijing 100083)(Manuscript received 1995-03-31; in revised form 1995-06-29) |
引用本文:
纪松;杨国斌;王润. Fe_(73.5)Cu_(1.0)Mo_(3.0)Si_(13.5)B_(9.0)纳米软磁合金的结构与磁性[J]. 金属学报, 1996, 32(1): 69-74.
,
,
.
MICROSTRUCTURE AND MAGNETIC PROPERTIES OF NANOSTRUCTURED SOFT MAGNETIC ALLOY Fe_(73.5) Cu_(1 .0)Mo_(3.0)Si_(13.5)B_(9.0)[J]. Acta Metall Sin, 1996, 32(1): 69-74.
| 1YoshizawaY,OyumaS,YamauchiK.JApplPhys,1988;64(10):60442裴光文,钟维烈,岳书彬.单晶、多晶和非晶物质的X射线衍射.济南:山东大学出版社,1986:4463张湘义,纪松.物理测试,1993;5:2034YelsukovYEP,BarinovVA,KonyginGN.PhysMetMetall,1986;64(6):855LiebermannHH,MartiJ,MartisRJ,WongCP.MetallTransA,1989;20A:636何开元.第六届全国非晶态材料和物理学术讨论会论文集,桂林,1991:1547王一禾,杨膺善.非晶态合金.北京:冶金工业出版社,1989:1558许裕生,吴名,瞿锋,徐松,高凤.第八届全国磁学磁性材料会议文集,烟台,1993:5079纪松,杨国斌,王润.94′秋季中国材料研讨会论文摘要集,北京,1994:61910ThomasAP,GibbsMRJ.JMagMagMater,1992:103:9711GengnagelH,WagnerH.ZAngewPhys,1961;4:17412沈德芳,井良文.物理学进展,1982;2(4):43513戴道生,钱昆明.铁磁学(上册),北京:科学出版社,1987:13814何开元.精密合金材料学.北京:冶金工业出版社,1991:6215NavarroI,PulidoE,CrespoP,HernandoA.JApplPhys,1993;73(10):6525 |
|