| 相场法模拟不同形状的硬质颗粒对两相晶粒长大的影响 |
| 周广钊,王永欣,陈铮 |
| 西北工业大学凝固技术国家重点实验室, 西安 710072 |
|
| PHASE–FIELD METHOD SIMULATION OF THE EFFECT OF HARD PARTICLES WITH DIFFERENT SHAPES ON TWO–PHASE GRAIN GROWTH |
| ZHOU Guangzhao, WANG Yongxin, CHEN Zheng |
| State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi’an 710072 |
引用本文:
周广钊 王永欣 陈铮. 相场法模拟不同形状的硬质颗粒对两相晶粒长大的影响[J]. 金属学报, 2012, 48(2): 227-234.
,
,
.
PHASE–FIELD METHOD SIMULATION OF THE EFFECT OF HARD PARTICLES WITH DIFFERENT SHAPES ON TWO–PHASE GRAIN GROWTH[J]. Acta Metall Sin, 2012, 48(2): 227-234.
| [1] Ryum N, Hunderi O, Nes E. Scr Metall, 1983; 17: 1281[2] Moelans N, Blanpain B, Wollants. Acta Mater, 2006; 54: 1175[3] Doherty R D, Srolovitz D J, Rollett A D, Anderson M P. Scr Metall, 1987; 21: 675[4] Hassold G N, Holm E A, Srolovitz D J. Scr Metall, 1990; 24: 101[5] Miodownik M, Holm E A, Hassold G N. Scr Metall, 2000; 42: 1173[6] AndersonM P, Grest G S, Doherty R D, Kang Li, Srolovitz D J. Scr Metall, 1989; 23: 753[7] Liu Z Y, Zheng Z Q, Chen D Q, Li S C. Chin J Nonferrous Met, 2004; 14: 122(刘祖耀, 郑子樵, 陈大钦, 李世晨. 中国有色金属学报, 2004; 14: 122)[8] Zhang J X, Guan X J. Chin J Nonferrous Met, 2006; 16: 1689(张继祥, 关小军. 中国有色金属学报, 2006; 16: 1689)[9] Song X Y, Liu G Q, Gu N J. Acta Metall Sin, 1999; 35: 565(宋晓艳, 刘国权, 谷南驹. 金属学报,1999; 35: 565)[10] Moelans N, Blanpain B, Wollants P. Calphad, 2008; 32: 268[11] Suwa Y, Saito Y, Onodera H. Scr Mater, 2006; 55: 407[12] Suwa Y, Satio Y, Onodera H. Acta Mater, 2007; 55: 6881[13] Vanherpe L, Moelans N, Blanpain B, Vandewalle S. Phys Rev, 2007; 76E: 056702[14] Vanherpe L, Moelans N, Blanpain B, Vandewalle S. Comput Mater Sci, 2010; 49: 340[15] Moelans N, Blanpain B, Wollants P. Acta Mater, 2007; 55: 2173[16] Li J J, Wang J C, Yang G C. Rare Met Mater Eng, 2008; 37: 1746(李俊杰, 王锦程, 杨根仓. 稀有金属材料与工程, 2008; 37: 1746)[17] Long Y Q, Liu P, Liu Y, Pan J S. Chin J Nonferrous Met, 2009; 19: 84(龙永强, 刘平, 刘勇, 潘健生. 中国有色金属学报, 2009; 19: 84)[18] Long Z R, Gao Y J, Qiu H G, Zhang H L. Chin J Nonferrous Met, 2010; 20: 2406(罗志荣, 高英俊, 邱鸿广, 张海林.中国有色金属学报, 2010; 20: 2406)[19] GaoY J, Zhang H L, Jin X, Huang C G, Luo Z R. Acta Metall Sin, 2009; 45: 1190(高英俊, 张海林, 金 \ \ 星, 黄创高, 罗志荣. 金属学报, 2009; 45: 1190)[20] Fan D, Chen L Q. Acta Metall, 1997; 45: 3297[21] Fan D, Chen L Q. Acta Metall, 1997; 45: 4145[22] Fan D, Chen L Q. J Am Ceram Soc, 1997; 80: 1773[23] Fan D, Chen L Q. J Am Ceram Soc, 1998; 81: 526[24] Song K, Aindow M. Mater Sci Eng, 2008; A479: 365[25] Ringer S P, Li W B, Easterling K E. Acta Metall, 1989; 37: 831[26] Li W B, Easterling K E. Acta Metall, 1990; 38; 1045[27] Cherukuri B, Srinivasan R, Tamirisakandala S, Miracle D B. Scr Mater, 2009; 60: 496[28] Ringer S P, Li W B, Easterling K E. Acta Metall, 1992; 40: 275[29] Ringer S P, Li W B, Easterling K E. in Chandra ed., Recrystallization’ 90 in Metals and Materials. Warrendale, PA: TMS–AIME, 1990; 26: 483 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|