基于机器学习的生物可降解锌合金力学性能预测
郭传平, 石尘尘, 刘鹏, 高冬芳, 赵洋洋, 乔阳

Prediction of Mechanical Properties of Biodegradable Zinc Alloys Based on Machine Learning
GUO Chuanping, SHI Chenchen, LIU Peng, GAO Dongfang, ZHAO Yangyang, QIAO Yang
表3 KNN算法验证集的预测值与实验值对比[19,26,27]
Table 3 Comparisons of prediction results of validation sets by KNN algorithm and experimental values[19,26,27]
No.Processing techniqueMgMnPredicted valueExperimental valueRef.
%%

CYS

MPa

Hardness

HV

CYS

MPa

Hardness

HV

1PM1.100.852007920381This work
2PM2.751.02201120198120This work
3PM1.570.421908418984This work
4PM0.520.15221118216115This work
5PM0.220.521906319364This work
6Cast1.000.10-92-98[19]
7Cast1.500.10-154-149
8HE00.401365613658[26]
9Cast1.200-85-93[27]