基于机器学习的生物可降解锌合金力学性能预测
郭传平, 石尘尘, 刘鹏, 高冬芳, 赵洋洋, 乔阳

Prediction of Mechanical Properties of Biodegradable Zinc Alloys Based on Machine Learning
GUO Chuanping, SHI Chenchen, LIU Peng, GAO Dongfang, ZHAO Yangyang, QIAO Yang
表1 用于制备Zn-Mg-Mn合金的粉末参数
Table 1 Powder parameters for the preparation of Zn-Mg-Mn alloy
PowderShapeParticle size / μmPurity %Melting point / oC
ZnSphericity< 3099.9419.5
MgSphericity≤ 4099.9648.9
MnIrregular shape< 3099.91244.0