基于机器学习的生物可降解锌合金力学性能预测
郭传平, 石尘尘, 刘鹏, 高冬芳, 赵洋洋, 乔阳

Prediction of Mechanical Properties of Biodegradable Zinc Alloys Based on Machine Learning
GUO Chuanping, SHI Chenchen, LIU Peng, GAO Dongfang, ZHAO Yangyang, QIAO Yang
图10 不同Mg含量下Zn-3.5Mn-xMg合金的力学性能、XRD谱及OM和SEM像
Fig.10 Mechanical properties (a), XRD patterns (b), and OM (c1, c2) and SEM (c3, c4) images of Zn-3.5Mn-xMg alloys (Red circles in Figs.10c2-c4 represent Mg2Zn11 phases)
(c1) Mg = 0 (c2) Mg = 1.0% (c3) Mg = 1.5% (c4) Mg = 2.5%